Polyoxometalate and method for producing polyoxometalate

US10647589B2 · US · B2

Patent metadata
FieldValue
Publication numberUS-10647589-B2
Application numberUS-201615563443-A
CountryUS
Kind codeB2
Filing dateMar 30, 2016
Priority dateMar 31, 2015
Publication dateMay 12, 2020
Grant dateMay 12, 2020

How to read this patent

A practical reading order for non-experts. Skip the full description unless you need deep technical detail.

  1. Title

    What the patent document calls the invention.

  2. Abstract

    A short plain-language summary of the technical disclosure.

  3. Assignees and inventors

    Who owns or filed the patent and who is credited as inventor.

  4. Key dates

    Filing, priority, publication, and grant dates set the timeline.

  5. First independent claim

    The legal scope of protection — read this for what is actually claimed.

  6. CPC / IPC classifications

    Technology tags used to group this patent with similar filings.

  7. Citations and related patents

    Prior art links and similar publications in this corpus.

Abstract

Official abstract text for this publication.

Provided is a novel polyoxometalate and a method for producing the polyoxometalate. The polyoxometalate is represented by the compositional formula: M x O y in which M is tungsten, molybdenum or vanadium; 4≤x≤1000; and 2.5≤y/x≤7.

First claim

Opening claim text (preview).

What is claimed is: 1. A method for producing a polyoxometalate, comprising: subjecting a raw material mixture comprising at least one valuable containing tungsten, molybdenum or vanadium to electrolysis using an organic electrolytic solution containing at least one alcohol amine to dissolve tungsten, molybdenum or vanadium in the electrolytic solution; and adding a poor solvent including an alcohol, an acetone, an ether, an amine or an ester to the electrolytic solution in which tungsten, molybdenum or vanadium has been dissolved, to produce a precipitate of a polyoxometalate of tungsten, molybdenum or vanadium. 2. The method for producing the polyoxometalate according to claim 1 , wherein the at least one alcohol amine is monoethanolamine and/or triethanolamine. 3. The method for producing the polyoxometalate according to claim 1 , wherein a concentration of the alcohol amine in the electrolytic solution is from 1 to 80% by mass. 4. The method for producing the polyoxometalate according to claim 1 , wherein the raw material mixture contains from 1 to 30% by mass of at least one valuable other than tungsten, molybdenum or vanadium. 5. The method for producing the polyoxometalate according to claim 4 , wherein the raw material mixture contains from 1 to 10% by mass of at least one valuable other than tungsten, molybdenum or vanadium. 6. The method for producing the polyoxometalate according to claim 5 , wherein the raw material mixture contains from 3 to 10% by mass of at least one valuable other than tungsten, molybdenum or vanadium. 7. The method for producing the polyoxometalate according to claim 1 , wherein the electrolysis is carried out by adjusting a temperature of the electrolytic solution to 20 to 80° C. 8. The method for producing the polyoxometalate according to claim 1 , wherein the electrolytic solution has a pH of 7 or more. 9. The method for producing the polyoxometalate according to claim 1 , wherein an anode used for the electrolysis is a titanium basket provided with the raw material mixture containing the at least one valuable containing tungsten, molybdenum or vanadium. 10. The method for producing the polyoxometalate according to claim 1 , wherein the organic electrolytic solution is an organic alkaline electrolytic solution. 11. The method for producing the polyoxometalate according to claim 2 , wherein a concentration of the alcohol amine in the electrolytic solution is from 1 to 80% by mass. 12. The method for producing the polyoxometalate according to claim 1 , wherein the raw material mixture contains from 1 to 30% by mass of at least one valuable other than tungsten. 13. The method for producing the polyoxometalate according to claim 1 , wherein the raw material mixture contains from 1 to 30% by mass of at least one valuable other than molybdenum. 14. The method for producing the polyoxometalate according to claim 1 , wherein the raw material mixture contains from 1 to 30% by mass of at least one valuable other than vanadium. 15. The method for producing the polyoxometalate according to claim 2 , wherein the raw material mixture contains from 1 to 30% by mass of at least one valuable other than tungsten, molybdenum or vanadium.

Assignees

Inventors

Classifications

  • Oxides · CPC title

  • Oxynitrides of metals, boron or silicon · CPC title

  • Compounds containing vanadium, with or without oxygen or hydrogen, and containing two or more other elements · CPC title

  • Electrodes (consumable anodes for the refining the metals C25C1/00 - C25C5/00); Connections thereof · CPC title

  • Compounds containing molybdenum, with or without oxygen or hydrogen, and containing two or more other elements · CPC title

Patent family

Related publications grouped by family.

External sources

Frequently asked questions

Answers are generated from the same data shown on this page.

What does patent US10647589B2 cover?
Provided is a novel polyoxometalate and a method for producing the polyoxometalate. The polyoxometalate is represented by the compositional formula: M x O y in which M is tungsten, molybdenum or vanadium; 4≤x≤1000; and 2.5≤y/x≤7.
Who is the assignee on this patent?
Jx Nippon Mining & Metals Corp
What technology area does this patent fall under?
Primary CPC classification C01B21/0821. Mapped technology areas include Chemistry & Metallurgy.
When was this patent published?
Publication date Tue May 12 2020 00:00:00 GMT+0000 (Coordinated Universal Time) (B2). Legal status and post-grant events are not shown on this page.