Cement set activators for set-delayed cement compositions and associated methods
US-9371712-B2 · Jun 21, 2016 · US
US9920235B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9920235-B2 |
| Application number | US-201615162245-A |
| Country | US |
| Kind code | B2 |
| Filing date | May 23, 2016 |
| Priority date | Mar 9, 2012 |
| Publication date | Mar 20, 2018 |
| Grant date | Mar 20, 2018 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Disclosed herein are cement compositions and methods of using set-delayed cement compositions in subterranean formations. In one embodiment, a method of cementing in a subterranean formation is described. The method may comprise providing a set-delayed cement composition comprising water, pumice, hydrated lime, and a set retarder; activating the set-delayed cement composition with a liquid additive to produce an activated cement composition, wherein the liquid additive comprises a monovalent salt, a polyphosphate, a dispersant, and water; and allowing the activated cement composition to set.
Opening claim text (preview).
What is claimed is: 1. A method of making an activated cement composition, the method comprising: providing a set-delayed cement composition comprising: water; pumice; hydrated lime; a set retarder selected from the group consisting of diethylenetriaminepentamethylenephosphonate, nitrilotrismethylenetriphosphonate, methylene phosphonates, methylene phosphonic acid derivatives, and combinations thereof; and adding a liquid activator to the set-delayed cement composition, wherein the liquid activator comprises water, a dispersant, a monovalent salt, and a polymeric metaphosphate salt. 2. The method of claim 1 wherein the polymeric metaphosphate salt comprises sodium hexametaphosphate. 3. The method of claim 1 wherein the monovalent salt comprises sodium sulfate. 4. The method of claim 1 wherein the dispersant comprises a polycarboxylated ether dispersant. 5. A method of making an activated cement composition, the method comprising: providing a set-delayed cement composition comprising: water; pumice; hydrated lime; and a set retarder selected from the group consisting of diethylenetriaminepentamethylenephosphonate, nitrilotrismethylenetriphosphonate, methylene phosphonates, methylene phosphonic acid derivatives, and combinations thereof; storing the set-delayed cement composition in a pumpable fluid state for at least about one day; and adding a liquid activator to the set-delayed cement composition, wherein the liquid activator comprises water, a dispersant, a polymeric metaphosphate salt and monovalent salt. 6. The method of claim 5 , wherein the dispersant is present in an amount in a range of about 0.01% to about 5% by weight of pumice. 7. The method of claim 5 wherein the set retarder is present in an amount in a range of about 0.01% to about 10% by weight of pumice. 8. The method of claim 5 wherein the hydrated lime is present in a range of about 10% to about 100% by weight of pumice. 9. The method of claim 5 wherein the water is present in an amount in the range of about 33% to about 200% by weight of pumice. 10. The method of claim 5 wherein the polymeric metaphosphate salt comprises sodium hexametaphosphate. 11. The method of claim 5 wherein a pumice-to-hydrated-lime weight ratio of about 10:1 to about 1:1. 12. The method of claim 5 wherein the water is present in an amount sufficient to form a pumpable slurry. 13. The method of claim 5 wherein a ratio of the monovalent salt to the polymeric metaphosphate salt is about 5:1 to about 1:25. 14. An activated cement composition comprising: water; pumice; hydrated lime; a set retarder selected from the group consisting of diethylenetriaminepentamethylenephosphonate, nitrilotrismethylenetriphosphonate, methylene phosphonates, methylene phosphonic acid derivatives, and combinations thereof; and a liquid activator, wherein the liquid activator comprises water polymeric metaphosphate salt, a dispersant, and a monovalent salt.
for cementing casings into boreholes · CPC title
Plastering the borehole wall; Injecting into the formation · CPC title
for squeeze cementing, e.g. for repairing · CPC title
Retarder inhibited mortars activated by the addition of accelerators or retarder-neutralising agents · CPC title
Microsilica, e.g. colloïdal silica (preparing microsilica slurries or suspensions C04B18/148) · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.