Cement set activators for set-delayed cement compositions and associated methods
US-9371712-B2 · Jun 21, 2016 · US
US10160900B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10160900-B2 |
| Application number | US-201415500428-A |
| Country | US |
| Kind code | B2 |
| Filing date | Sep 30, 2014 |
| Priority date | Sep 30, 2014 |
| Publication date | Dec 25, 2018 |
| Grant date | Dec 25, 2018 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Methods of using the set-delayed cement slurries and compositions resulting from the combination of the set-delayed cement slurries are also described. A method may comprise providing a first set-delayed cement slurry comprising a pozzolanic cement and/or a Portland cement, water, and a first cement set retarder; providing a second set-delayed cement slurry comprising calcium-aluminate and a second cement set retarder; mixing the first slurry and the second slurry to form a cement composition; and allowing the cement composition to set.
Opening claim text (preview).
What is claimed is: 1. A method of cementing comprising: providing a first set-delayed cement slurry comprising a cement selected from the group consisting of a pozzolanic cement, a Portland cement, and combinations thereof, water, and a first cement set retarder wherein the first set-delayed cement slurry is capable of remaining in a pumpable fluid state for at least about 7 days at room temperature in quiescent storage; providing a second set-delayed cement slurry comprising calcium-aluminate and a second cement set retarder wherein the second cement set retarder is different than the first cement set retarder and wherein the second set-delayed cement slurry is capable of remaining in a pumpable fluid state for at least about 7 days at room temperature in quiescent storage; mixing the first set-delayed cement slurry and the second set-delayed cement slurry to form an activated cement composition; and thereafter, allowing the cement composition to set to form a hardened mass. 2. The method according to claim 1 wherein the cement composition is introduced into a wellbore penetrating a subterranean formation after the step of mixing, and allowed to set within. 3. The method according to claim 1 , wherein the first set-delayed cement slurry comprises the pozzolanic cement and wherein the pozzolanic cement is selected from the group consisting of fly ash, silica fume, metakaolin, pumice, and any combination thereof. 4. The method according claim 1 , wherein the first set-delayed cement slurry comprises the pozzolanic cement and lime. 5. The method according to claim 1 , wherein the cement composition further comprises at least one dispersant selected from the group consisting of a sulfonated-formaldehyde-based dispersant, a polycarboxylated ether dispersant, and any combination thereof. 6. The method according to claim 1 , wherein at least one of the first cement set retarder or the second cement set retarder is selected from the group consisting of a phosphonic acid, a phosphonic acid derivative, a lignosulfonate, a salt, an organic acid, a carboxymethylated hydroxyethylated cellulose, a synthetic co- or ter-polymer comprising sulfonate and carboxylic acid groups, a borate compound, and any combination thereof. 7. The method according to claim 1 , further comprising storing at least one of the first set-delayed cement slurry or the second set-delayed cement slurry for a time period of about 1 day or longer prior to the step of mixing. 8. The method according to claim 1 , further comprising storing at least one of the first set-delayed cement slurry or the second set-delayed cement slurry for a time period of about 7 days or longer prior to the step of mixing. 9. The method according to claim 1 , wherein at least one of the first set-delayed cement slurry or the second set-delayed cement slurry comprises a lithium salt. 10. The method according to claim 1 , further comprising pumping the cement composition through a feed pipe and into a wellbore annulus that is penetrating a subterranean formation after the step of mixing. 11. The method according to claim 1 , further comprising introducing at least a portion of the first set-delayed cement slurry into a wellbore that penetrates a subterranean formation such that the first set-delayed cement slurry displaces at least one fluid from the wellbore. 12. A method of making a cement composition, the method comprising: preparing a first set-delayed cement slurry comprising a cement selected from the group consisting of a pozzolanic cement, a Portland cement, and combinations thereof, water, and a first cement set retarder and storing the first set-delayed cement slurry for a period of about 1 day or longer; preparing a second set-delayed cement slurry comprising calcium-aluminate and a second cement set retarder and storing the second set-delayed cement slurry for a period of about 1 day or longer; and mixing the first set-delayed cement slurry and the second set-delayed cement slurry to form an activated cement composition. 13. The method according to claim 12 , wherein the cement composition comprises the pozzolanic cement and wherein the pozzolanic cement is selected from the group consisting of fly ash, silica fume, metakaolin, pumice, and any combination thereof. 14. The method according to claim 12 , wherein the cement composition further comprises a dispersant. 15. The method according to claim 14 , wherein the dispersant comprises at least one dispersant selected from the group consisting of a sulfonated-formaldehyde-based dispersant, a polycarboxylated ether dispersant, and any combination thereof. 16. The method according to claim 12 , wherein at least one of the first cement set retarder or the second cement set retarder is selected from the group consisting of a phosphonic acid, a phosphonic acid derivative, a lignosulfonate, a salt, an organic acid, a carboxymethylated hydroxyethylated cellulose, a synthetic co- or ter-polymer comprising sulfonate and carboxylic acid groups, a borate compound, and any combination thereof. 17. The method according to claim 12 , wherein the cement composition further comprises a lithium salt. 18. A system for cementing comprising: a first set-delayed cement slurry comprising a cement selected from the group consisting of a pozzolanic cement, a Portland cement, and combinations thereof, water, and a first cement set retarder wherein the first set-delayed cement slurry is capable of remaining in a pumpable fluid state for a period of about 1 day or longer; a second set-delayed cement slurry comprising calcium-aluminate and a second cement set retarder wherein the second set-delayed cement slurry is capable of remaining in a pumpable fluid state for a period of about 1 day or longer; a first vessel capable of containing the first slurry, wherein the first vessel also comprises a first pump capable of pumping the first slurry; a second vessel capable of containing the second slurry, wherein the second vessel also comprises a second pump capable of pumping the second slurry; a line connected to the first pump and the second pump, wherein the line is capable of mixing the first set-delayed cement slurry and the second set-delayed cement slurry to form an activated cement composition; and a third pump connected to the line capable of delivering the activated cement composition into a wellbore. 19. The system according to claim 18 , wherein at least one of the first cement set retarder or the second cement set retarder is selected from the group consisting of a phosphonic acid, a phosphonic acid derivative, a lignosulfonate, a salt, an organic acid, a carboxymethylated hydroxyethylated cellulose, a synthetic co- or ter-polymer comprising sulfonate and carboxylic acid groups, a borate compound, and any combination thereof. 20. The system according to claim 18 , wherein at least one of the first set-delayed cement slurry or the second set-delayed cement slurry comprises a lithium salt.
Flue dust {, i.e. fly ash} · CPC title
Condensation {or polymerisation} products thereof · CPC title
Lignin sulfonic acid or derivatives thereof, e.g. sulfite lye · CPC title
Boron compounds · CPC title
containing polyether side chains · CPC title