Set-delayed cement compositions comprising pumice and associated methods

US9878949B2 · US · B2

Patent metadata
FieldValue
Publication numberUS-9878949-B2
Application numberUS-201615087961-A
CountryUS
Kind codeB2
Filing dateMar 31, 2016
Priority dateMar 9, 2012
Publication dateJan 30, 2018
Grant dateJan 30, 2018

How to read this patent

A practical reading order for non-experts. Skip the full description unless you need deep technical detail.

  1. Title

    What the patent document calls the invention.

  2. Abstract

    A short plain-language summary of the technical disclosure.

  3. Assignees and inventors

    Who owns or filed the patent and who is credited as inventor.

  4. Key dates

    Filing, priority, publication, and grant dates set the timeline.

  5. First independent claim

    The legal scope of protection — read this for what is actually claimed.

  6. CPC / IPC classifications

    Technology tags used to group this patent with similar filings.

  7. Citations and related patents

    Prior art links and similar publications in this corpus.

Abstract

Official abstract text for this publication.

Disclosed herein are cement compositions and methods of using set-delayed cement compositions in subterranean formations. An embodiment includes a method of cementing in a subterranean formation comprising: providing a cement composition comprising water, pumice, hydrated lime, a set retarder, and a strength enhancer, wherein the strength enhancer comprises at least one material selected from the group consisting of cement kiln dust, slag, amorphous silica, a pozzolan, and any combination thereof; introducing the cement composition into the subterranean formation; and allowing the cement composition to set in the subterranean formation.

First claim

Opening claim text (preview).

What is claimed is: 1. A cement composition created by a process comprising the steps of: providing a set-delayed cement composition comprising: water; pumice; hydrated lime; a polycarboxylate ether dispersant; and a phosphonic acid set retarder; adding a liquid additive activator to the set-delayed cement composition, the liquid additive activator comprising: a monovalent salt; a polyphosphate; a dispersant; and a strength enhancer, wherein the strength enhancer is selected from the group consisting of cement kiln dust, slag, amorphous silica diatomaceous earth, metakaolin, fly ash, zeolite, and combinations thereof. 2. The composition of claim 1 wherein the strength enhancer is the cement kiln dust and wherein the cement kiln dust is present in an amount of about 50% to about 100% by weight of the pumice. 3. The composition of claim 1 wherein the strength enhancer is the slag and wherein the slag is present in an amount of about 50% to about 100% by weight of the pumice. 4. The composition of claim 1 wherein the strength enhancer is the amorphous silica and wherein the amorphous silica is present in an amount of about 0.1% to about 20% by weight of the pumice. 5. The composition of claim 1 wherein the strength enhancer is the diatomaceous earth, metakaolin, fly ash, zeolite, and combinations thereof; and wherein the strength enhancer is present in an amount of about 0.1% to about 20% by weight of the pumice. 6. The composition of claim 1 wherein the set retarder further comprises at least one retarder selected from the group consisting of a phosphate, a phosphonate, a phosphonic acid derivative, a lignosulfonate, a salt, an organic acid, a carboxymethylated hydroxyethylated cellulose, a synthetic co- or ter-polymer comprising sulfonate and carboxylic acid groups, a borate compound, and any mixture thereof. 7. The composition of claim 1 wherein the set retarder is present in an amount of about 0.01% to about 10% by weight of the pumice. 8. The composition of claim 1 wherein the liquid additive activator is added in an amount of about 0.1% to about 20% by weight of the pumice. 9. The composition of claim 1 wherein the set-delayed cement composition is capable of remaining in a pumpable fluid state for a period of about 1 day or longer. 10. The composition of claim 1 wherein the composition further comprises a sulfonated-formaldehyde-based dispersant. 11. The composition of claim 10 wherein the polycarboxylate ether dispersant and the sulfonated-formaldehyde-based dispersant are present in a total amount of about 0.01% to about 5% by weight of the pumice. 12. A method of preparing a cement composition comprising: providing a set-delayed cement composition comprising: pumice; hydrated lime; a dispersant; and a retarder; wherein the set delayed cement composition is capable of remaining in a pumpable fluid state for at least about one day or longer; allowing the set-delayed cement composition to remain in quiescent storage for about one day; adding a liquid additive the set-delayed cement composition, the liquid additive comprising: water; a cement set activator; and a strength enhancer. 13. The method of claim 12 wherein the dispersant comprises a at least one dispersant selected from the group consisting of a sulfonated-formaldehyde-based dispersant, a polycarboxylated ether dispersant, and combinations thereof. 14. The dispersant of claim 13 wherein the dispersant is present in an amount of about 0.01% to about 5% by weight of the pumice. 15. The method of claim 12 wherein the set retarder comprises at least one retarder selected from the group consisting of a phosphate, a phosphonate, a phosphonic acid, a phosphonic acid derivative, a lignosulfonate, a salt, an organic acid, a carboxymethylated hydroxyethylated cellulose, a synthetic co- or ter-polymer comprising sulfonate and carboxylic acid groups, a borate compound, and any mixture thereof. 16. The method of claim 12 wherein the cement set activator comprises at least one set activator selected from the group consisting of zeolites, amines, silicates, Groups IA and IIA hydroxides, monovalent salts, divalent salts, nanosilica, polyphosphates, and combinations thereof. 17. The method of claim 12 wherein the strength enhancer is selected from the group consisting of cement kiln dust, slag, amorphous silica, diatomaceous earth, metakaolin, fly ash, zeolite, and combinations thereof. 18. The method of claim 17 wherein the strength enhancer comprises the slag and wherein the slag is present in an amount of about 50% to about 100% by weight of the pumice. 19. The method of claim 17 wherein the strength enhancer comprises the amorphous silica and wherein the amorphous silica is present in an amount of about 0.1% to about 20% by weight of the pumice. 20. The method of claim 12 wherein the liquid additive is added in an amount of about 0.1% to about 20% by weight of the pumice. 21. A cement composition comprising: pumice; hydrated lime, wherein the hydrated lime is present in a pumice-to-hydrated-lime weight ratio of about 3:1 to about 5:1; a phosphonic acid set retarder; a polycarboxylated ether dispersant; a suspension aid; a calcium chloride activator; cement kiln dust present in an amount of about 1% to about 10% by weight of the pumice; a weighting agent; and water.

Assignees

Inventors

Classifications

  • porous, e.g. pumice · CPC title

  • C04B28/10Primary

    Lime cements or magnesium oxide cements · CPC title

  • containing additives for specific purposes · CPC title

  • Cross-Sectional Technologies · mapped topic

  • Dispersants · CPC title

Patent family

Related publications grouped by family.

External sources

Frequently asked questions

Answers are generated from the same data shown on this page.

What does patent US9878949B2 cover?
Disclosed herein are cement compositions and methods of using set-delayed cement compositions in subterranean formations. An embodiment includes a method of cementing in a subterranean formation comprising: providing a cement composition comprising water, pumice, hydrated lime, a set retarder, and a strength enhancer, wherein the strength enhancer comprises at least one material selected from t…
Who is the assignee on this patent?
Halliburton Energy Services Inc, Hallliburton Energy Services Inc
What technology area does this patent fall under?
Primary CPC classification C04B28/10. Mapped technology areas include Chemistry & Metallurgy.
When was this patent published?
Publication date Tue Jan 30 2018 00:00:00 GMT+0000 (Coordinated Universal Time) (B2). Legal status and post-grant events are not shown on this page.
What related patents are in patentsdb?
We list 9 related publications on this page (citations in our corpus or others sharing the same primary CPC).