Set-delayed cement compositions comprising pumice and associated methods

US9790132B2 · US · B2

Patent metadata
FieldValue
Publication numberUS-9790132-B2
Application numberUS-201514634764-A
CountryUS
Kind codeB2
Filing dateFeb 28, 2015
Priority dateMar 9, 2012
Publication dateOct 17, 2017
Grant dateOct 17, 2017

How to read this patent

A practical reading order for non-experts. Skip the full description unless you need deep technical detail.

  1. Title

    What the patent document calls the invention.

  2. Abstract

    A short plain-language summary of the technical disclosure.

  3. Assignees and inventors

    Who owns or filed the patent and who is credited as inventor.

  4. Key dates

    Filing, priority, publication, and grant dates set the timeline.

  5. First independent claim

    The legal scope of protection — read this for what is actually claimed.

  6. CPC / IPC classifications

    Technology tags used to group this patent with similar filings.

  7. Citations and related patents

    Prior art links and similar publications in this corpus.

Abstract

Official abstract text for this publication.

Disclosed is a method of spraying a surface with a set-delayed cement. The method comprises providing a set-delayed cement composition comprising water, pumice, hydrated lime, and a set retarder; spraying a surface with the set-delayed cement composition; and allowing the set-delayed cement composition to set on the surface.

First claim

Opening claim text (preview).

What is claimed is: 1. A method of spraying a surface with a set-delayed cement composition, the method comprising: providing a set-delayed cement composition comprising water, pumice, hydrated lime, and a set retarder; conveying the set-delayed cement composition though a conduit and a nozzle; activating the set-delayed cement composition with a cement set activator within the nozzle to produce an activated cement composition, wherein the activating the set-delayed cement composition comprises contacting the set-delayed cement composition and the cement set activator within the nozzle, wherein the activator is provided in an amount such that the activated cement composition has a thickening time in a range of about 30 seconds to about 10 minutes; spraying a surface with the activated cement composition; and allowing the activated cement composition to set on the surface. 2. The method of claim 1 wherein the set retarder comprises at least one retarder selected from the group consisting of a phosphate, a phosphonate, a phosphonic acid, a phosphonic acid derivative, a lignosulfonate, a salt, an organic acid, a carboxymethylated hydroxyethylated cellulose, a synthetic co- or ter-polymer comprising sulfonate and carboxylic acid groups, a borate compound, and any mixture thereof. 3. The method of claim 1 wherein the cement set activator selected from the group consisting of a zeolite, amine, silicate, Group IA hydroxide, Group IIA hydroxide, monovalent salt, divalent salt, nanosilica, polyphosphate, and any combination thereof. 4. The method of claim 1 wherein the set-delayed cement composition further comprises a fiber. 5. The method of claim 1 wherein the set-delayed cement composition further comprises a dispersant selected from the group consisting of a sulfonated-formaldehyde-based dispersant, a polycarboxylated ether dispersant, and any combination thereof. 6. The method of claim 1 further comprising, prior to the spraying step, storing the set-delayed cement composition for a period of at least about 1 day. 7. The method of claim 1 , wherein the surface is disposed about, on, or within a mine, a pond, a creek, a river, the ocean floor, a beach shore, a wall, a ceiling, a floor, an attic, or a basement. 8. The method of claim 1 , wherein the set-delayed cement composition is disposed within a mine and wherein the set-delayed cement composition is pumped from a vessel outside of the mine into the mine. 9. The method of claim 1 , wherein the set-delayed cement composition is foamed. 10. The method of claim 1 , wherein the set-delayed cement composition comprises refractory materials. 11. The method of claim 1 , wherein the set-delayed cement composition comprises a dye and/or beads. 12. A method of coating a surface with a set-delayed cement composition, the method comprising: providing a set-delayed cement composition comprising water, pumice, hydrated lime, and a set retarder; conveying the set-delayed cement composition though a nozzle and conduit wherein the nozzle is coupled to the conduit; activating the set-delayed cement composition with a Group IA hydroxide, Group IIA hydroxide, or combinations thereof to produce an activated cement composition; coating a surface with the activated cement composition; and allowing the activated cement composition to set on the surface. 13. The method of claim 12 wherein the set retarder comprises at least one retarder selected from the group consisting of a phosphate, a phosphonate, a phosphonic acid, a phosphonic acid derivative, a lignosulfonate, a salt, an organic acid, a carboxymethylated hydroxyethylated cellulose, a synthetic co- or ter-polymer comprising sulfonate and carboxylic acid groups, a borate compound, and any mixture thereof. 14. The method of claim 12 wherein the cement set activator further comprises an activator selected from the group consisting of a zeolite, amine, silicate, monovalent salt, divalent salt, nanosilica, polyphosphate, and any combination thereof. 15. The method of claim 12 wherein the activated cement composition comprises a thickening time in a range between about 30 seconds to about 10 minutes. 16. The method of claim 12 wherein the coating a surface with the activated cement composition comprises painting the surface with the set-delayed cement composition or dipping the surface into a vessel containing the activated cement composition.

Assignees

Inventors

Classifications

  • C04B28/18Primary

    containing mixtures of the silica-lime type · CPC title

  • containing additives for specific purposes · CPC title

  • Retarder inhibited mortars activated by the addition of accelerators or retarder-neutralising agents · CPC title

  • Coating or impregnating "in situ", e.g. impregnating of artificial stone by subsequent melting of a compound added to the artificial stone composition · CPC title

  • Porous mortars, concrete, artificial stone or ceramic ware; Preparation thereof (treating slag with gases or gas generating material C04B5/06 {; expanded graphite C04B35/536}) · CPC title

Patent family

Related publications grouped by family.

External sources

Frequently asked questions

Answers are generated from the same data shown on this page.

What does patent US9790132B2 cover?
Disclosed is a method of spraying a surface with a set-delayed cement. The method comprises providing a set-delayed cement composition comprising water, pumice, hydrated lime, and a set retarder; spraying a surface with the set-delayed cement composition; and allowing the set-delayed cement composition to set on the surface.
Who is the assignee on this patent?
Halliburton Energy Services Inc
What technology area does this patent fall under?
Primary CPC classification C04B28/18. Mapped technology areas include Chemistry & Metallurgy.
When was this patent published?
Publication date Tue Oct 17 2017 00:00:00 GMT+0000 (Coordinated Universal Time) (B2). Legal status and post-grant events are not shown on this page.
What related patents are in patentsdb?
We list 9 related publications on this page (citations in our corpus or others sharing the same primary CPC).