Method for producing colored wood

US12459159B2 · US · B2

Patent metadata
FieldValue
Publication numberUS-12459159-B2
Application numberUS-202218273570-A
CountryUS
Kind codeB2
Filing dateJan 24, 2022
Priority dateJan 26, 2021
Publication dateNov 4, 2025
Grant dateNov 4, 2025

How to read this patent

A practical reading order for non-experts. Skip the full description unless you need deep technical detail.

  1. Title

    What the patent document calls the invention.

  2. Abstract

    A short plain-language summary of the technical disclosure.

  3. Assignees and inventors

    Who owns or filed the patent and who is credited as inventor.

  4. Key dates

    Filing, priority, publication, and grant dates set the timeline.

  5. First independent claim

    The legal scope of protection — read this for what is actually claimed.

  6. CPC / IPC classifications

    Technology tags used to group this patent with similar filings.

  7. Citations and related patents

    Prior art links and similar publications in this corpus.

Abstract

Official abstract text for this publication.

Provided is a method for producing colored wood, the method including: a step of impregnating a block of wood with an organic acid aqueous solution containing an organic acid; and a step of performing steam treatment at high temperature and high pressure on the block of wood in a wet state of being impregnated with the organic acid aqueous solution while keeping the block of wood in the wet state. In the steam treatment, the temperature is 110° C. or more and 160° C. or less and the pressure is a saturated steam pressure at the temperature.

First claim

Opening claim text (preview).

The invention claimed is: 1 . A method for producing colored wood, the method comprising: impregnating a block of wood with an organic acid aqueous solution containing an organic acid, wherein the wood is artificially dried wood, a moisture content of the artificially dried wood is 7% to 25%, and the moisture content of the wood is measured in accordance with the Japanese Industrial Standard JIS Z2101; and performing steam treatment at a temperature and a pressure on the block of wood in a wet state of being impregnated with the organic acid aqueous solution while keeping the block of wood in the wet state, wherein, in the steam treatment, the temperature is 110° C. or more and 160° C. or less and the pressure is a saturated steam pressure at the temperature, and wherein a thickness of the wood is 10 mm or more and 40 mm or less. 2 . The method for producing colored wood according to claim 1 , wherein the organic acid aqueous solution further contains a saccharide. 3 . The method for producing colored wood according to claim 2 , wherein the saccharide is at least one selected from the group consisting of fructose, maltose, xylose, and sucrose. 4 . The method for producing colored wood according to claim 2 , wherein in the organic acid aqueous solution, an amount of the saccharide is 3% to 30% by mass. 5 . The method for producing colored wood according to claim 1 , wherein the organic acid is a divalent or higher carboxylic acid. 6 . The method for producing colored wood according to claim 5 , wherein the carboxylic acid is at least one selected from the group consisting of citric acid, malic acid, and succinic acid. 7 . The method for producing colored wood according to claim 1 , wherein in the organic acid aqueous solution, an amount of the organic acid is 3% to 30% by mass. 8 . The method for producing colored wood according to claim 1 , the method further comprising: drying the block of wood that has been subjected to the steam treatment. 9 . The method for producing colored wood according to claim 1 , the method further comprising: obtaining a sliced veneer by slicing the block of wood that has been subjected to the steam treatment. 10 . The method for producing colored wood according to claim 8 , the method further comprising: after drying the block of wood that has been subjected to the steam treatment, heating the block of wood under an inert atmosphere. 11 . The method for producing colored wood according to claim 10 , wherein the inert atmosphere is a nitrogen atmosphere or a superheated steam atmosphere.

Assignees

Inventors

Classifications

  • Aliphatic compounds · CPC title

  • using pressure (B27K3/08 takes precedence) · CPC title

  • Damping wood · CPC title

  • involving an additional treatment during or after impregnation · CPC title

  • Heating · CPC title

Patent family

Related publications grouped by family.

External sources

Frequently asked questions

Answers are generated from the same data shown on this page.

What does patent US12459159B2 cover?
Provided is a method for producing colored wood, the method including: a step of impregnating a block of wood with an organic acid aqueous solution containing an organic acid; and a step of performing steam treatment at high temperature and high pressure on the block of wood in a wet state of being impregnated with the organic acid aqueous solution while keeping the block of wood in the wet sta…
Who is the assignee on this patent?
Panasonic Ip Man Co Ltd
What technology area does this patent fall under?
Primary CPC classification B27K5/02. Mapped technology areas include Operations & Transport.
When was this patent published?
Publication date Tue Nov 04 2025 00:00:00 GMT+0000 (Coordinated Universal Time) (B2). Legal status and post-grant events are not shown on this page.
What related patents are in patentsdb?
We list 8 related publications on this page (citations in our corpus or others sharing the same primary CPC).