High-strength portland cement slurry for ultra-high temperature cementing, preparation method therefor and application thereof
US-2023278927-A1 · Sep 7, 2023 · US
US12378161B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-12378161-B2 |
| Application number | US-202117996717-A |
| Country | US |
| Kind code | B2 |
| Filing date | Apr 22, 2021 |
| Priority date | Apr 23, 2020 |
| Publication date | Aug 5, 2025 |
| Grant date | Aug 5, 2025 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A cement admixture containing free lime, gypsum, Ye'elimite, and ternesite, wherein the cement admixture has a mass ratio of the Ye'elimite to the ternesite (Ye'elimite/ternesite) of from 0.5 to 40. The cement admixture contains 20 to 80 mass % of the free lime. The cement admixture has a total mass ratio of the free lime and the gypsum anhydride to the ternesite ((free lime+gypsum anhydride)/ternesite) from 20 to 90. An expansive material which contains the cement admixture. A cement composition which contains the cement admixture.
Opening claim text (preview).
The invention claimed is: 1. A cement admixture, comprising free lime, gypsum anhydride, Ye'elimite, and ternesite, wherein a mass ratio of the Ye'elimite to the ternesite (Ye'elimite/ternesite) is 0.5 to 40. 2. The cement admixture according to claim 1 , wherein the cement admixture contains 20 to 80 mass % of the free lime. 3. The cement admixture according to claim 1 , wherein a total mass ratio of the free lime and the gypsum anhydride to the ternesite ((free lime+gypsum anhydride)/ternesite) is 20 to 90. 4. An expansive material comprising the cement admixture according to claim 1 . 5. A cement composition comprising the cement admixture according to claim 1 .
containing hydraulic cements other than calcium sulfates · CPC title
Oxides, Hydroxides (C04B22/0013 takes precedence) · CPC title
containing sulfur in the anion, e.g. sulfides · CPC title
Premixtures of ingredients · CPC title