Method for producing conjugated diolefin and apparatus for production
US-9255041-B2 · Feb 9, 2016 · US
US9790140B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9790140-B2 |
| Application number | US-201415021540-A |
| Country | US |
| Kind code | B2 |
| Filing date | Sep 9, 2014 |
| Priority date | Sep 12, 2013 |
| Publication date | Oct 17, 2017 |
| Grant date | Oct 17, 2017 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A method for producing butadiene from 2,3-butanediol with high selectivity without using a radioactive substance is disclosed. The method for producing butadiene comprises the step of dehydrating 2,3-butanediol in the presence of a catalyst containing an alkali metal salt of phosphoric acid such as an alkali metal dihydrogen phosphate supported on silica. Preferred examples of the alkali metal herein include K, Rb, and Cs. The catalyst is preferably a catalyst prepared by calcination of the silica to which the alkali metal of phosphoric acid is attached.
Opening claim text (preview).
The invention claimed is: 1. A method for producing butadiene, said method comprising dehydrating 2,3-butanediol in the presence of a catalyst containing an alkali metal dihydrogen phosphate supported on silica to produce a product stream containing butadiene. 2. The method according to claim 1 , wherein a weight ratio of said alkali metal dihydrogen phosphate to the total weight of said silica and said alkali metal dihydrogen phosphate in said catalyst is not less than 5 wt % and not more than 40 wt % before supporting said alkali metal dihydrogen phosphate on said silica. 3. The method according to claim 1 , wherein the alkali metal in said alkali metal dihydrogen phosphate is one or more selected from the group consisting of K, Rb, and Cs. 4. The method according to claim 1 , wherein said alkali metal dihydrogen phosphate is supported on said silica by calcination of silica to which alkali metal dihydrogen phosphate was attached. 5. The method according to claim 1 , wherein a reaction temperature of the dehydrating 2,3-butanediol is not less than 380° C. and not more than 520° C.
Drying, e.g. preparing a suspension, adding a soluble salt and drying · CPC title
Phosphates or other compounds comprising the anion (PnO3n+1)(n+2)- · CPC title
by elimination of water · CPC title
Phosphoric acid or other acids with the formula Hn+2PnO3n+1 · CPC title
Heat treatment {(B01J37/0009, B01J37/0018 take precedence)} · CPC title