Method of preparing iron oxide nanoparticles

US9755231B2 · US · B2

Patent metadata
FieldValue
Publication numberUS-9755231-B2
Application numberUS-201414248479-A
CountryUS
Kind codeB2
Filing dateApr 9, 2014
Priority dateJan 25, 2013
Publication dateSep 5, 2017
Grant dateSep 5, 2017

How to read this patent

A practical reading order for non-experts. Skip the full description unless you need deep technical detail.

  1. Title

    What the patent document calls the invention.

  2. Abstract

    A short plain-language summary of the technical disclosure.

  3. Assignees and inventors

    Who owns or filed the patent and who is credited as inventor.

  4. Key dates

    Filing, priority, publication, and grant dates set the timeline.

  5. First independent claim

    The legal scope of protection — read this for what is actually claimed.

  6. CPC / IPC classifications

    Technology tags used to group this patent with similar filings.

  7. Citations and related patents

    Prior art links and similar publications in this corpus.

Abstract

Official abstract text for this publication.

Provided are a method of preparing iron oxide nanoparticles, iron oxide nanoparticles prepared thereby, and an anode material including the iron oxide nanoparticles.

First claim

Opening claim text (preview).

What is claimed is: 1. A method of preparing oval shaped iron (III) oxide nanoparticles, the method comprising: preparing a ferric chloride (FeCl 3 ) aqueous solution; preparing a sodium hydroxide (NaOH) aqueous solution; obtaining a mixed aqueous solution consisting of the ferric chloride (FeCl 3 ) aqueous solution, the sodium hydroxide (NaOH) aqueous solution, and a sodium sulfate (Na 2 SO 4 ) aqueous solution; reacting the mixed aqueous solution in an electric convection oven in a temperature range of 100° C. to 105° C. for 90 hours to 100 hours at atmospheric pressure to get a solid product; and cooling, washing, and drying the solid product to get a dried product, wherein a concentration of the FeCl 3 aqueous solution is in a range of 2 M to 3 M, a concentration of the NaOH aqueous solution is in a range of 5 M to 6 M, a concentration of the Na 2 SO 4 aqueous solution is in a range of 0.5 M to 1 M, and the dried product consists of iron (III) oxide. 2. The method of claim 1 , wherein a volume ratio of the ferric chloride aqueous solution:the sodium hydroxide aqueous solution:the sodium sulfate aqueous solution is 10:9:x, where x satisfies 0<x<1.

Assignees

Inventors

Classifications

  • extending in three dimensions · CPC title

  • H01M4/521Primary

    of iron for aqueous cells · CPC title

  • Iron electrodes · CPC title

  • Physical characteristics, e.g. porosity, surface area · CPC title

  • Submicrometer sized, i.e. from 0.1-1 micrometer · CPC title

Patent family

Related publications grouped by family.

External sources

Frequently asked questions

Answers are generated from the same data shown on this page.

What does patent US9755231B2 cover?
Provided are a method of preparing iron oxide nanoparticles, iron oxide nanoparticles prepared thereby, and an anode material including the iron oxide nanoparticles.
Who is the assignee on this patent?
Lg Chemical Ltd
What technology area does this patent fall under?
Primary CPC classification H01M4/521. Mapped technology areas include Electricity.
When was this patent published?
Publication date Tue Sep 05 2017 00:00:00 GMT+0000 (Coordinated Universal Time) (B2). Legal status and post-grant events are not shown on this page.
What related patents are in patentsdb?
We list 8 related publications on this page (citations in our corpus or others sharing the same primary CPC).