Non-lithium metal ion battery electrode material architecture

US9725331B2 · US · B2

Patent metadata
FieldValue
Publication numberUS-9725331-B2
Application numberUS-201414274169-A
CountryUS
Kind codeB2
Filing dateMay 9, 2014
Priority dateMay 10, 2013
Publication dateAug 8, 2017
Grant dateAug 8, 2017

How to read this patent

A practical reading order for non-experts. Skip the full description unless you need deep technical detail.

  1. Title

    What the patent document calls the invention.

  2. Abstract

    A short plain-language summary of the technical disclosure.

  3. Assignees and inventors

    Who owns or filed the patent and who is credited as inventor.

  4. Key dates

    Filing, priority, publication, and grant dates set the timeline.

  5. First independent claim

    The legal scope of protection — read this for what is actually claimed.

  6. CPC / IPC classifications

    Technology tags used to group this patent with similar filings.

  7. Citations and related patents

    Prior art links and similar publications in this corpus.

Abstract

Official abstract text for this publication.

A method for configuring a non-lithium-intercalation electrode includes intercalating an insertion species between multiple layers of a stacked or layered electrode material. The method forms an electrode architecture with increased interlayer spacing for non-lithium metal ion migration. A laminate electrode material is constructed such that pillaring agents are intercalated between multiple layers of the stacked electrode material and installed in a battery.

First claim

Opening claim text (preview).

We claim: 1. A battery electrode architecture comprising: a layered structure comprising A x M y N Z , a pillaring agent, and at least one non-lithium metal ion X n+ , wherein, in a first state, the layered structure comprises a first layer of A x M y N Z a second layer of A x M y N Z , and a spacing between the first and the second layers, wherein the pillaring agent and the non-lithium metal ion are disposed between the first layer and the second layer of the A x M y N Z ; wherein, in a second state, subsequent to a plurality of battery electrode cycles, the pillaring agent remains disposed between the first and second layers and the layered structure is configured to maintain the spacing of the first state; wherein A is at least one low-valence element selected from the group consisting of H, alkaline, and alkaline earth metals, and 0≦x≦1.5; M is at least one metal and 1≦y≦2.5; N is at least one non-metal element selected from the group consisting of O, S, Se, N, F, Br, and I; and 1.8≦z≦4.2; and X n+ is at least one non-lithium metal ion selected from the group consisting of Na, K, Mg, Ca, Al, Ga, and Y, and 1≦n≦3. 2. The battery electrode architecture of claim 1 , wherein a low-valence element further comprises at least one chosen from the group consisting of Li, Na, K, Mg, and Ca. 3. The battery electrode architecture of claim 1 wherein the at least one metal comprises a metal selected from the group consisting of Ti, Zr, V, Ta, Cr, Mo, W, Mn, Fe, Ni, Co, Cu, Zn, Cd, Ga, In, Sn, Pb, Sb, Bi, and Te. 4. The battery electrode architecture of claim 1 , wherein the pillaring agent comprises at least one electrically neutral polymer containing O, N, F, or S atoms. 5. The battery electrode architecture of claim 4 , wherein the at least one electrically neutral polymer comprises at least one polymer selected from the group consisting of poly(ethylene oxide), poly(propylene glycol), poly(vinylpyrrolidinone), methyl cellulose, poly(methyl acrylate), polyacrylonitrile, polyethyleneimine, poly(aniline), and polypyrrole. 6. The battery electrode architecture of claim 4 , wherein the pillaring agent comprises at least one molecule selected from the group consisting of alkylamines and glymes. 7. The battery electrode architecture of claim 6 , wherein the alkylamines comprise of at least one molecule selected from the group consisting of diethylamine, dibutylamine, dipentylamine, N-isopropylcyclohexyl amine, and dicyclohexylamine. 8. The battery electrode architecture of claim 6 , wherein the glymes consist of at least one molecule selected from the group consisting of diglyme, triglyme, and tetraglyme. 9. The battery electrode architecture of claim 1 , wherein the non-lithium metal ion X n+ is positioned within the lattice spacing of A x M y N z . 10. The battery electrode architecture of claim 9 , wherein the at least one electrically neutral polymer and the non-lithium metal ion X n+ in the lattice spacing of A x M y N z induce a lattice expansion of 1-300% in at least one dimension. 11. The battery electrode architecture of claim 1 , wherein the spacing is from about 6 Angstroms to about 25 Angstroms. 12. A battery electrode architecture comprising: a layered structure comprising A x M y N z , a pillaring agent, and at least one non-lithium metal ion X n+ , wherein, in a first state, the layered structure comprises a first layer of A x M y N z a second layer of A x M y N z , and a spacing between the first and the second layers, wherein the pillaring agent and the non-lithium metal ion are disposed between the first layer and the second layer of the A x M y N z , wherein, in a second state, wherein, in a second state, subsequent to a plurality of battery electrode cycles, the pillaring agent remains disposed between the first and second layers and the layered structure is configured to maintain the spacing of the first state, and wherein X n+ comprises Mg 2+ or Al 3+ . 13. The architecture of claim 12 , further comprising wherein A is at least one low-valence element selected from the group consisting of H, alkaline, and alkaline earth metals, and 0≦x≦1.5. 14. The architecture of claim 12 , further comprising 1≦y≦2.5. 15. The architecture of claim 12 , further comprising wherein N is at least one non-metal element selected from the group consisting of O, S, Se, N, P, Br, and I, and 1.8≦z≦4.2. 16. A battery electrode architecture comprising: a layered structure comprising A x M y N z , a pillaring agent, and at least one non-lithium metal ion X n+ , wherein, in a first state, the layered structure comprises a first layer of A x M y N z a second layer of A x M y N z , and a spacing between the first and the second layers from about 6 Angstroms to about 25 Angstroms, wherein the pillaring agent and the non-lithium metal ion are disposed between the first layer and the second layer of the A x M y N z , wherein, in a second state, wherein, in a second state, subsequent to a plurality of battery electrode cycles, the pillaring agent remains disposed between the first and second layers and the layered structure is configured to maintain the spacing of the first state, and wherein X n+ comprises a polarization strength of at least 40×10 −5 pm −2 . 17. The architecture of claim 16 , further comprising wherein A is at least one low-valence element selected from the group consisting of H, alkaline, and alkaline earth metals, and 0≦x≦1.5. 18. The architecture of claim 16 , further comprising 1≦y≦2.5. 19. The architecture of claim 16 , further comprising wherein N is at least one non-metal element selected from the group consisting of O, S, Se, N, P, Br, and I, and 1.8≦z≦4.2.

Assignees

Inventors

Classifications

  • by d-values or two theta-values, e.g. as X-ray diagram · CPC title

  • of elements or alloys · CPC title

  • Sulfides · CPC title

  • Selection of substances as active materials, active masses, active liquids · CPC title

  • Electric properties · CPC title

Patent family

Related publications grouped by family.

External sources

Frequently asked questions

Answers are generated from the same data shown on this page.

What does patent US9725331B2 cover?
A method for configuring a non-lithium-intercalation electrode includes intercalating an insertion species between multiple layers of a stacked or layered electrode material. The method forms an electrode architecture with increased interlayer spacing for non-lithium metal ion migration. A laminate electrode material is constructed such that pillaring agents are intercalated between multiple la…
Who is the assignee on this patent?
Univ Houston System
What technology area does this patent fall under?
Primary CPC classification C01G39/06. Mapped technology areas include Chemistry & Metallurgy.
When was this patent published?
Publication date Tue Aug 08 2017 00:00:00 GMT+0000 (Coordinated Universal Time) (B2). Legal status and post-grant events are not shown on this page.
What related patents are in patentsdb?
We list 8 related publications on this page (citations in our corpus or others sharing the same primary CPC).