Thermoplastic resin composition for refrigerant transporting piping, and method for producing same
US-12071541-B2 · Aug 27, 2024 · US
US9708464B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9708464-B2 |
| Application number | US-201314386420-A |
| Country | US |
| Kind code | B2 |
| Filing date | Mar 22, 2013 |
| Priority date | Mar 23, 2012 |
| Publication date | Jul 18, 2017 |
| Grant date | Jul 18, 2017 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A rubber-metal composite body constituted of a rubber composition and a metal material embedded therein is conventionally used in a rubber article requiring high strength in order to reinforce rubber to improve strength and durability thereof. The present invention provides a rubber composition having good initial adhesive properties and good heat resistant adhesive properties with respect to a metal material, mainly for use in the rubber-metal composite body as described above. Specifically, the present invention provides a rubber composition, containing a cobalt compound by an amount, according to cobalt atoms, in the range of 0.0025 to 0.05 parts by mass with respect to 100 parts by mass of a rubber component.
Opening claim text (preview).
The invention claimed is: 1. A method for manufacturing a rubber-metal composite body, comprising: a surface treatment process comprising bringing a metal material into contact with a buffer solution for 0.5 second to 20 seconds, the buffer solution being free of cobalt and substantially free of transition metals; and a bonding process comprising bonding the metal material subjected to the surface treatment process to a rubber composition containing a cobalt compound in an amount, according to cobalt atoms, in the range of 0.0025 to 0.025 parts by mass with respect to 100 parts by mass of a rubber component and containing no nickel and molybdenum. 2. The method for manufacturing a rubber-metal composite body of claim 1 , wherein the pH of the buffer solution is set to be in the range of 5.0 to 7.2. 3. The method for manufacturing a rubber-metal composite body of claim 1 , wherein the buffer solution contains at least one type of acid selected from acids each having an acid dissociation constant (pKa) in the range of 4 to 8.
Metal salts of carboxylic acids · CPC title
with all layers existing as coherent layers before laminating · CPC title
of continuously flexible type, e.g. rubber belts · CPC title
Other operations not otherwise provided for · CPC title
Compositions of unspecified rubbers · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.