Novel copolymer with cyclic halamine structure
US-2016297911-A1 · Oct 13, 2016 · US
US9458255B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9458255-B2 |
| Application number | US-201013260907-A |
| Country | US |
| Kind code | B2 |
| Filing date | Mar 29, 2010 |
| Priority date | Mar 31, 2009 |
| Publication date | Oct 4, 2016 |
| Grant date | Oct 4, 2016 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
The present invention is aimed to provide a highly-productive method for producing a stabilized fluoropolymer. The present invention relates to a method for producing a stabilized fluoropolymer, comprising the step of bringing a fluoropolymer to be treated into contact with a fluorinating agent to produce a stabilized fluoropolymer, while maintaining the concentration of hydrogen fluoride present in a reaction vessel at not higher than 1.0% by volume.
Opening claim text (preview).
The invention claimed is: 1. A method for producing a stabilized fluoropolymer, comprising the step of bringing a fluoropolymer to be treated into contact with a fluorinating agent in a stationary reactor to produce a stabilized fluoropolymer, while maintaining the concentration of hydrogen fluoride present in a reaction vessel at not higher than 1.0% by volume, wherein the contacting step is carried out at a temperature of 50° C. or higher and 185° C. or lower, and the fluoropolymer to be treated is in the form of a resin powder, a pellet, or a membrane obtained through molding, and the fluoropolymer to be treated is constituted by 50 to 100 mol % of an ethylenic fluoromonomer unit and 0 to 50 mol % of a fluorinated alkyl vinyl ether unit, and the fluoropolymer to be treated has an unstable group and the unstable group is at least one group selected from the group consisting of —CF 2 COF, —CF 2 COOH, —CF 2 CH 2 OH, —CF 2 COOCH 3 , and —COOCO—, wherein —CF 2 COF —CF 2 COOH, —CF 2 CH 2 OH and —CF 2 COOCH 3 are terminal groups and wherein —COOCO— represents a group formed by bonding two —CF 2 COOH terminal groups. 2. The method for producing a stabilized fluoropolymer according to claim 1 , wherein the fluorinating agent is at least one substance selected from the group consisting of F 2 , NF 3 , SF 4 , ClF, ClF 3 , BrF 3 , and IF 5 . 3. The method for producing a stabilized fluoropolymer according to claim 1 , wherein the fluorinating agent is F 2 . 4. The method for producing a stabilized fluoropolymer according to claim 1 , wherein the contacting step is carried out at a temperature of 50° or higher and 120° or lower.
Monomers containing fluorine · CPC title
Halogenation · CPC title
Monomers containing fluorine · CPC title
by reaction with free halogens · CPC title