Dense packing particle size distribution for pdc cutters
US-2015375366-A1 · Dec 31, 2015 · US
US9388331B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9388331-B2 |
| Application number | US-201214369915-A |
| Country | US |
| Kind code | B2 |
| Filing date | Dec 14, 2012 |
| Priority date | Dec 28, 2011 |
| Publication date | Jul 12, 2016 |
| Grant date | Jul 12, 2016 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Provided is a method for manufacturing an abrasive agent including a dispersant and also including cerium oxide as a main abrasive material component. The method involves: a step for recovering an abrasive agent component by salting out a spent abrasive material slurry by using a cation of an element of the first Group or second Group with an ionic radius of 80 pm to 160 pm in six-coordinate conversion, and solid-liquid separating the cerium oxide by coagulation and sedimentation; and a step for adding a dispersant including an anionic polymer to the abrasive agent component after the recovery.
Opening claim text (preview).
The invention claimed is: 1. A method for manufacturing an abrasive agent comprising a dispersant and further including cerium oxide as a main abrasive material component, the method comprising: recovering an abrasive agent component by salting out a spent abrasive material slurry by using a cation which is at least one cation selected from the group consisting of a magnesium ion and a calcium ion, wherein said cation has an ionic radius of 80 pm to 160 pm in six-coordinate conversion, and solid-liquid separating the cerium oxide by coagulation and sedimentation; and adding a dispersant including an anionic polymer to the abrasive agent component after the recovery. 2. The method for manufacturing an abrasive agent according to claim 1 , wherein the cation has an ionic radius of 80 pm to 120 pm in six-coordinate conversion. 3. The method for manufacturing an abrasive agent according to claim 1 , wherein the dispersant is a polymer having a carboxyl group in a molecule. 4. The method for manufacturing an abrasive agent according to claim 3 , wherein the dispersant is an acrylic acid/maleic acid copolymer with a weight-average molecular weight (Mw) of 100 to 10,000. 5. The method for manufacturing an abrasive agent according to claim 1 , wherein the amount of the dispersant added is 0.05% by mass to 2% by mass with respect to a total amount of the abrasive agent.
Abrasive particles per se (preparation of diamond C01B32/25) · CPC title
Aqueous liquid suspensions · CPC title
Non-aqueous liquid suspensions · CPC title