Emulsion and mold-releasing agent using the same
US-9610634-B2 · Apr 4, 2017 · US
US9259862B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9259862-B2 |
| Application number | US-201213590889-A |
| Country | US |
| Kind code | B2 |
| Filing date | Aug 21, 2012 |
| Priority date | Aug 21, 2012 |
| Publication date | Feb 16, 2016 |
| Grant date | Feb 16, 2016 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A method of molding a plastic container body having at least one grip recess includes providing a mold assembly having an internal projection that is constructed and arranged to form the grip recess. A low friction surface is provided on at least a portion of the projection in order to reduce friction between the formable plastic material and the projection during the molding process. The low friction surface permits the formable plastic material to stretch with less resistance before it solidifies to the point where additional stretching is not possible. As a result, molding of features that provide resistance to material distribution during molding, such as deep grip recesses, is enabled.
Opening claim text (preview).
What is claimed is: 1. A method of making a plastic container having a container body with a grip recess defined therein, comprising: providing a mold assembly that defines an internal mold surface, the internal mold surface having a first surface portion that has a first frictional coefficient, the internal mold surface further having a projection configured to form a grip recess, the projection in transverse cross-section includes a first side surface, a second side surface, and an apex defined between the first and second side surfaces, wherein at least a portion of the first side surface of the projection defines a low friction second surface portion that has a second frictional coefficient that is less than the first frictional coefficient; applying formable plastic material against the internal mold surface to form a container body having at least one grip recess; and removing the container body from the mold. 2. A method of making a plastic container according to claim 1 , wherein the mold assembly has a longitudinal axis that corresponds to a longitudinal axis of the container, and wherein the first side surface defines a first angle with respect to a first radius extending from the longitudinal axis and the second side surface defines a second angle with respect to a second radius extending from the longitudinal axis, and wherein the second angle is greater than the first angle. 3. A method of making a plastic container according to claim 2 , wherein the low friction second surface portion includes at least a portion of the apex. 4. A method of making a plastic container according to claim 1 , wherein the low friction second surface portion comprises a layer of low friction material that is attached to an underlying mold surface. 5. A method of making a plastic container according to claim 4 , further comprising applying the layer of low friction material to at least a portion of the projection by a spraying process. 6. A method of making a plastic container according to claim 1 , further comprising inspecting the low friction second surface portion. 7. A method of making a plastic container according to claim 6 , further comprising performing maintenance on the low friction second surface portion based on results of the inspection. 8. A method of making a plastic container according to claim 4 , wherein the low friction material comprises a fluoropolymer. 9. A mold assembly for forming a plastic container having a container body with a grip recess defined therein, comprising: structure defining an internal mold surface, the internal mold surface having a first surface portion that has a first frictional coefficient; and a projection configured to form a grip recess, the projection as viewed in transverse cross-section including a first side surface, a second side surface, and an apex defined between the first and second side surfaces, wherein at least a portion of the first side surface of the projection defines a low friction second surface portion that has a second frictional coefficient that is less than the first frictional coefficient. 10. A mold assembly according to claim 9 , wherein the mold assembly has a longitudinal axis that corresponds to a longitudinal axis of the container, and wherein the first side surface defines a first angle with respect to a first radius extending from the longitudinal axis and the second side surface defines a second angle with respect to a second radius extending from the longitudinal axis, and wherein the second angle is greater than the first angle. 11. A mold assembly according to claim 10 , wherein the low friction second surface portion includes at least a portion of the apex. 12. A mold assembly according to claim 9 , wherein the low friction second surface portion comprises a layer of low friction material that is attached to an underlying mold surface. 13. A mold assembly according to claim 12 , wherein the layer of low friction material comprises a sprayable material. 14. A mold assembly according to claim 12 , wherein the low friction material comprises a fluoropolymer. 15. A mold assembly according to claim 9 , wherein the internal mold surface is constructed and arranged to form a plastic container body having an outermost periphery as viewed in transverse cross-section that is substantially round. 16. A method of making a plastic container according to claim 1 , wherein the first surface portion of the internal mold surface having the first friction coefficient includes at least a portion of the second side surface of the projection. 17. A mold assembly according to claim 9 , wherein the first surface portion of the internal mold surface having the first friction coefficient includes at least a portion of the second side surface of the projection.