Method for recovering active metal of lithium secondary battery
US-12542310-B2 · Feb 3, 2026 · US
US9233419B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9233419-B2 |
| Application number | US-201313968770-A |
| Country | US |
| Kind code | B2 |
| Filing date | Aug 16, 2013 |
| Priority date | Oct 17, 2008 |
| Publication date | Jan 12, 2016 |
| Grant date | Jan 12, 2016 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
The invention relates to a process for producing sinterable molybdenum metal powder in a moving bed, sinterable molybdenum powder and its use.
Opening claim text (preview).
The invention claimed is: 1. Molybdenum metal powder which has a specific surface area, measured in accordance with ASTM 3663, of from 0.5 to 2 m 2 /g, a flowability of ≧140 sec per 50 g of powder, measured in accordance with ASTM B 213, and an oxygen content of from 0.07 to 0.5%. 2. Molybdenum metal powder according to claim 1 , wherein the powder has an FSSS/FSSS lab milled ratio of ≧1.4 and ≦5. 3. Molybdenum metal powder according to claim 1 , wherein the powder has an FSSS/FSSS lab milled ratio of ≧1.4 and ≦3. 4. Molybdenum metal powder according to claim 1 , wherein the powder has an FSSS/FSSS lab milled ratio of ≧1.4 and ≦2.5. 5. Molybdenum metal powder according to claim 1 , wherein the FSSS particle size of the powder, measured in accordance with ASTM B 330, is from 2 to 8 μm. 6. Molybdenum metal powder according to claim 1 , wherein the FSSS particle size of the powder, measured in accordance with ASTM B 330, is from 2 to 7 μm. 7. Molybdenum metal powder according to claim 1 , wherein the FSSS particle size of the powder, measured in accordance with ASTM B 330, is from 3 to 5 μm. 8. Molybdenum metal powder according to claim 1 , wherein the powder has a specific surface area, measured in accordance with ASTM 3663, of from 0.5 to 1.5 m 2 /g. 9. Molybdenum metal powder according to claim 1 , wherein the powder has a specific surface area, measured in accordance with ASTM 3663, of from 0.5 to 1.2 m 2 /g. 10. Molybdenum metal powder according to claim 1 , wherein the powder has a specific surface area, measured in accordance with ASTM 3663, of from 0.5 to 1.0 m 2 /g. 11. Molybdenum metal powder according to claim 1 , wherein the powder has a specific surface area, measured in accordance with ASTM 3663, of from 0.5 to 0.8 m 2 /g. 12. Molybdenum metal powder according to claim 1 , wherein the powder has an oxygen content of from 0.07 to 0.3%. 13. Molybdenum metal powder according to claim 1 , wherein the powder has an oxygen content of from 0.07 to 0.1%. 14. Molybdenum metal powder according to claim 1 , wherein the powder has an oxygen content of from 0.08 to 0.1%. 15. Molybdenum metal powder according to claim 1 , wherein the powder has a tapped density, measured in accordance with ASTM B 527, of from 1.8 to 2.6 g/cm 3 .
using gaseous reductors · CPC title
Hydrogen · CPC title
Alloys based on tungsten or molybdenum · CPC title
Refractory metals · CPC title