Single crystal cathode materials using microwave plasma processing

US2026015760A1 · US · A1

Patent metadata
FieldValue
Publication numberUS-2026015760-A1
Application numberUS-202519040742-A
CountryUS
Kind codeA1
Filing dateJan 29, 2025
Priority dateJan 19, 2021
Publication dateJan 15, 2026
Grant date

How to read this patent

A practical reading order for non-experts. Skip the full description unless you need deep technical detail.

  1. Title

    What the patent document calls the invention.

  2. Abstract

    A short plain-language summary of the technical disclosure.

  3. Assignees and inventors

    Who owns or filed the patent and who is credited as inventor.

  4. Key dates

    Filing, priority, publication, and grant dates set the timeline.

  5. First independent claim

    The legal scope of protection — read this for what is actually claimed.

  6. CPC / IPC classifications

    Technology tags used to group this patent with similar filings.

  7. Citations and related patents

    Prior art links and similar publications in this corpus.

Abstract

Official abstract text for this publication.

Disclosed herein are systems and methods for synthesis of submicron-scale or micron-scale single crystal cathode (SCC) material, such as NMC, using a feedstock and microwave plasma processing. Microwave plasma processing of these SCC materials provides a low cost, scalable approach. In some embodiments, advanced SCC materials may be synthesized through microwave plasma processing of feedstock materials, wherein the SCC materials may comprise at least 80% nickel. In some embodiments, the microwave plasma processing may enable synthesis of SCC materials with very short calcination.

First claim

Opening claim text (preview).

What is claimed is: 1 . A method for synthesizing single-crystal lithium-ion cathode (SCC) material, the method comprising: providing a solid or liquid feedstock, the feedstock comprising lithium and nickel; introducing the feedstock into a microwave-generated plasma to produce a solid precursor of SCC material, wherein introducing the feedstock into the microwave-generated plasma comprises feeding the feedstock to the microwave-generated plasma downstream in a plume or exhaust of the microwave-generated plasma; and calcining the solid precursor of SCC material to produce the SCC material, wherein the solid precursor of SCC material comprises metal oxide and unreacted lithium nitrate. 2 . The method of claim 1 , wherein the SCC material comprises a lithium nickel cobalt manganese oxide (NMC) powder. 3 . The method of claim 2 , wherein the NMC powder comprises NMC-811. 4 . The method of claim 2 , wherein the NMC powder comprises at least 80% nickel by weight. 5 . The method of claim 1 , wherein the solid precursor of SCC material comprises NMC having pores filled with lithium nitrate. 6 . The method of claim 1 , wherein the feedstock comprises lithium, nickel, and cobalt nitrate or lithium, nickel, and cobalt acetate salts dissolved in water. 7 . The method of claim 1 , wherein the SCC material comprises an agglomerated SCC material and the method further comprises deagglomerating the agglomerated SCC material to produce SCC powder. 8 . The method of claim 1 , further comprising adding lithium or lithium salt to the solid precursor of SCC material prior to or during calcining the solid precursor of SCC material. 9 . The method of claim 1 , wherein lithium nitrate is located within pores of the precursor of SCC material. 10 . The method of claim 1 , wherein the solid precursor of SCC material is calcined for about 0.25 hours to about 10 hours at a temperature between about 650° C. and 1000° C. 11 . The method of claim 1 , wherein the solid precursor of SCC material comprising metal oxide and unreacted lithium nitrate comprises inhomogeneous material with lithiated metal oxides and unreacted lithium nitrate intimate with one another in clumps. 12 . The method of claim 11 , wherein the clumps comprise nanoparticles. 13 . The method of claim 12 , wherein the nanoparticles have diameters of less than about 900 nm. 14 . The method of claim 1 , wherein the solid precursor of SCC material comprises a disordered but layered NMC structure. 15 . The method of claim 1 , wherein the solid precursor of SCC material comprises a disordered but non-layered structure. 16 . The method of claim 5 , wherein the majority of lithium in the feedstock does not react to leave lithium nitrate in the solid precursor of SCC.

Assignees

Inventors

Classifications

  • of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy · CPC title

  • of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy · CPC title

  • Positive electrodes · CPC title

  • C30B29/22Primary

    Complex oxides · CPC title

  • Energy storage using batteries · CPC title

Patent family

Related publications grouped by family.

External sources

Frequently asked questions

Answers are generated from the same data shown on this page.

What does patent US2026015760A1 cover?
Disclosed herein are systems and methods for synthesis of submicron-scale or micron-scale single crystal cathode (SCC) material, such as NMC, using a feedstock and microwave plasma processing. Microwave plasma processing of these SCC materials provides a low cost, scalable approach. In some embodiments, advanced SCC materials may be synthesized through microwave plasma processing of feedstock m…
Who is the assignee on this patent?
6K Inc
What technology area does this patent fall under?
Primary CPC classification C30B29/22. Mapped technology areas include Chemistry & Metallurgy.
When was this patent published?
Publication date Thu Jan 15 2026 00:00:00 GMT+0000 (Coordinated Universal Time) (A1). Legal status and post-grant events are not shown on this page.
What related patents are in patentsdb?
We list 8 related publications on this page (citations in our corpus or others sharing the same primary CPC).