Blends of polyarylene ethers and polyarylene sulfides
US-9212281-B2 · Dec 15, 2015 · US
US2022010131A1 · US · A1
| Field | Value |
|---|---|
| Publication number | US-2022010131-A1 |
| Application number | US-202117482938-A |
| Country | US |
| Kind code | A1 |
| Filing date | Sep 23, 2021 |
| Priority date | Mar 27, 2019 |
| Publication date | Jan 13, 2022 |
| Grant date | — |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A resin composition containing an aromatic polyether ketone resin (I); and a fluorine-containing copolymer (II), the resin composition satisfying an r2/r1 ratio of 1.60 or lower, wherein r1 is an average dispersed particle size of the fluorine-containing copolymer (II) and r2 is an average dispersed particle size of the fluorine-containing copolymer (II) after melt flow rate measurement at 380° C. and a load of 5000 g and with a preheating time of five minutes in conformity with ASTM D1238. Also disclosed is a pellet obtained by molding the resin composition and a molded article formed from the resin composition or the pellet.
Opening claim text (preview).
What is claimed is: 1 . A resin composition comprising: an aromatic polyether ketone resin (I); and a fluorine-containing copolymer (II), the resin composition satisfying an r2/r1 ratio of 1.60 or lower, wherein r1 is an average dispersed particle size of the fluorine-containing copolymer (II) and r2 is an average dispersed particle size of the fluorine-containing copolymer (II) after melt flow rate measurement at 380° C. and a load of 5000 g and with a preheating time of five minutes in conformity with ASTM D1238. 2 . The resin composition according to claim 1 , wherein the aromatic polyether ketone resin (I) has a melting point of 300° C. to 380° C. 3 . The resin composition according to claim 1 , wherein the aromatic polyether ketone resin (I) has a glass transition temperature of 130° C. to 220° C. 4 . The resin composition according to claim 1 , wherein the fluorine-containing copolymer (II) has a melting point of 200° C. to 323° C. 5 . The resin composition according to claim 1 , wherein the fluorine-containing copolymer (II) is a copolymer of tetrafluoroethylene and a perfluoroethylenic unsaturated compound represented by the following formula (1): CF 2 ═CF—Rf 1 (1) wherein Rf 1 is —CF 3 or —ORf 2 , where Rf 2 is a C1-C5 perfluoroalkyl group. 6 . The resin composition according to claim 1 , wherein the aromatic polyether ketone resin (I) and the fluorine-containing copolymer (II) are present in a mass ratio (I):(II) of 99:1 to 30:70. 7 . The resin composition according to claim 1 , further comprising a fibrous filler (III). 8 . A pellet obtained by molding the resin composition according to claim 1 . 9 . A molded article formed from the resin composition according to claim 1 . 10 . A molded article formed from the pellet according to claim 8 .
Related publications grouped by family.
Answers are generated from the same data shown on this page.