Particulate porous carbon material, particulate carbon material aggregate, and production method for particulate porous carbon material
US-2017291820-A1 · Oct 12, 2017 · US
US2021087717A1 · US · A1
| Field | Value |
|---|---|
| Publication number | US-2021087717-A1 |
| Application number | US-202017019526-A |
| Country | US |
| Kind code | A1 |
| Filing date | Sep 14, 2020 |
| Priority date | Sep 19, 2019 |
| Publication date | Mar 25, 2021 |
| Grant date | — |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A method of producing a stabilized fiber, including performing a heat treatment on an acrylamide polymer fiber under an oxidizing atmosphere in a stabilization treatment temperature range of 200° C. to 500° C. while applying a tension of 0.07 mN/tex to 15 mN/tex.
Opening claim text (preview).
What is claimed is: 1 . A method of producing a stabilized fiber, comprising performing a heat treatment on an acrylamide polymer fiber under an oxidizing atmosphere in a stabilization treatment temperature range of 200° C. to 500° C. while applying a tension of 0.07 mN/tex to 15 mN/tex. 2 . The method according to claim 1 , wherein the heat treatment is performed until an intensity ratio of a G peak near 1,590 cm −1 to a D peak near 1,360 cm −1 in a Raman spectrum on a side of the acrylamide polymer fiber becomes 0.5 or more. 3 . The method according to claim 1 , wherein the heat treatment is performed until a density of the acrylamide polymer fiber becomes 1.35 g/cm 3 to 1.75 g/cm 3 . 4 . A method of producing a carbon fiber, comprising: producing the stabilized fiber using the method according to claim 1 ; and performing carbonization on the stabilized fiber. 5 . A stabilized fiber which is derived from an acrylamide polymer and has an intensity ratio of 0.5 or more of a G peak near 1,590 cm −1 to a D peak near 1,360 cm −1 in a Raman spectrum on the side of the fiber. 6 . A method of producing a carbon fiber, comprising performing carbonization on the stabilized fiber according to claim 5 . 7 . A stabilized fiber which is derived from an acrylamide polymer and has a density of 1.35 g/cm 3 to 1.75 g/cm 3 . 8 . A method of producing a carbon fiber, comprising performing carbonization on the stabilized fiber according to claim 7 .
from macromolecular compounds obtained by reactions only involving carbon-to-carbon unsaturated bonds · CPC title
Heat treatment (heating for finishing D02J13/00) · CPC title
Carbon (carbon nanotubes C04B14/026) · CPC title
Carbon; Pitch · CPC title
from other polymers · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.