Oriented electrical steel sheet with excellent magnetic properties and method for manufacturing same
US-2017369959-A1 · Dec 28, 2017 · US
US2021039354A1 · US · A1
| Field | Value |
|---|---|
| Publication number | US-2021039354-A1 |
| Application number | US-201816979820-A |
| Country | US |
| Kind code | A1 |
| Filing date | Mar 20, 2018 |
| Priority date | Mar 20, 2018 |
| Publication date | Feb 11, 2021 |
| Grant date | — |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
There is provided a hot-stamped body including: a steel base metal; and a metallic layer formed on a surface of the steel base metal, wherein the metallic layer includes: an interface layer that contains, in mass %, Al: 30.0 to 36.0%, has a thickness of 100 nm to 5 μm, and is located in an interface between the metallic layer and the steel base metal; and a principal layer that includes coexisting MgZn 2 phases and insular FeAl 2 phases, is located on the interface layer, and has a thickness of 3 μm to 40 μm.
Opening claim text (preview).
1 . A hot-stamped body comprising: a steel base metal; and a metallic layer formed on a surface of the steel base metal, wherein the metallic layer includes an interface layer and a principal layer, the interface layer contains, in mass %, Al: 30.0 to 36.0%, has a thickness of 100 nm to 5 μm, and is located in an interface between the metallic layer and the steel base metal, the principal layer includes coexisting MgZn 2 phases and insular FeAl 2 phases, has a thickness of 3 μm to 40 μm, and is located on the interface layer, an average composition of the metallic layer consists of, in mass %: Al: 20.0 to 45.0%; Fe: 10.0 to 45.0%; Mg: 2.0 to 10.0%; Sb: 0 to 0.5%; Pb: 0 to 0.5%; Cu: 0 to 1.0%; Sn: 0 to 1.0%; Ti: 0 to 1.0%; Ca: 0 to 3.0%; Sr: 0 to 0.5%; Cr: 0 to 1.0%; Ni: 0 to 1.0%; Mn: 0 to 1.0%; Si: 0 to 1.0%; and the balance: 12.0 to 45.0% of Zn and impurities, in the principal layer, the MgZn 2 phases each contain, in mass %: Mg: 13.0 to 20.0%. Zn: 70.0 to 87.0%; Al: 0 to 8.0%; and Fe: 0 to 5.0%, and in the principal layer, the FeAl 2 phases each contain, in mass %: Al: 40.0 to 55.0%; Fe: 40.0 to 55.0%; and Zn: 0 to 15.0%. 2 . The hot-stamped body according to claim 1 , wherein in the principal layer, a volume fraction of the FeAl 2 phases is 50.0 to 80.0%, and a volume fraction of the MgZn 2 phases is 20.0 to 50.0%. 3 . The hot-stamped body according to claim 1 , wherein in the principal layer, a volume fraction of the FeAl 2 phases is 60.0 to 75.0%, and a volume fraction of the MgZn 2 phases is 25.0 to 45.0%. 4 . The hot-stamped body according to claim 2 , wherein in the principal layer, a volume fraction of the FeAl 2 phases is 60.0 to 75.0%, and a volume fraction of the MgZn 2 phases is 25.0 to 45.0%. 5 . A hot-stamped body comprising: a steel base metal; and a metallic layer formed on a surface of the steel base metal, wherein the metallic layer includes an interface layer and a principal layer, the interface layer contains, in mass %, Al: 30.0 to 36.0%, has a thickness of 100 nm to 5 μm, and is located in an interface between the metallic layer and the steel base metal, the principal layer includes coexisting MgZn 2 phases and insular FeAl 2 phases, has a thickness of 3 μm to 40 μm, and is located on the interface layer, an average composition of the metallic layer comprises, in mass %: Al: 20.0 to 45.0%; Fe: 10.0 to 45.0%; Mg: 2.0 to 10.0%; Sb: 0 to 0.5%; Pb: 0 to 0.5%; Cu: 0 to 1.0%; Sn: 0 to 1.0%; Ti: 0 to 1.0%; Ca: 0 to 3.0%; Sr: 0 to 0.5%; Cr: 0 to 1.0%; Ni: 0 to 1.0%; Mn: 0 to 1.0%; Si: 0 to 1.0%; and the balance: 12.0 to 45.0% of Zn and impurities, in the principal layer, the MgZn 2 phases each contain, in mass %: Mg: 13.0 to 20.0%. Zn: 70.0 to 87.0%; Al: 0 to 8.0%; and Fe: 0 to 5.0%, and in the principal layer, the FeAl 2 phases each contain, in mass %: Al: 40.0 to 55.0%; Fe: 40.0 to 55.0%; and Zn: 0 to 15.0%.
Modifying the physical properties of ferrous metals or ferrous alloys by deformation combined with, or followed by, heat treatment (hardening articles or materials formed by forging or rolling with no further heating beyond that required for the formation C21D1/02) · CPC title
Cooling or quenching · CPC title
Thermal after-treatment, e.g. treatment in oil bath · CPC title
in a gas atmosphere, e.g. inert or reducing atmosphere · CPC title
1 mil or less · CPC title