System and method for mandrel-less electrospinning
US-2017326772-A1 · Nov 16, 2017 · US
US2016303788A1 · US · A1
| Field | Value |
|---|---|
| Publication number | US-2016303788-A1 |
| Application number | US-201615131029-A |
| Country | US |
| Kind code | A1 |
| Filing date | Apr 18, 2016 |
| Priority date | Apr 20, 2015 |
| Publication date | Oct 20, 2016 |
| Grant date | — |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A method for manufacturing a bond magnet includes providing a bond magnet composition including a magnetic material and a resin, extruding the bond magnet composition in one direction to produce a molded body while orienting the magnetic material in the one direction, magnetizing the molded body in the one direction using an axial magnetization to produce a magnetized molded body, and laminating the magnetized molded body to produce a laminated molded body including first magnetized molded layers and second magnetized molded layers. The first magnetized molded layers and the second magnetized molded layers are alternately laminated. A first magnetization direction of each of the first magnetized molded layers is opposite to a second magnetization direction of each of the second magnetized molded layers.
Opening claim text (preview).
What is claimed is: 1 . A method for manufacturing a bond magnet, the method comprising: providing a bond magnet composition including a magnetic material and a resin; extruding the bond magnet composition in one direction to produce a molded body while orienting the magnetic material in the one direction; magnetizing the molded body in the one direction using an axial magnetization to produce a magnetized molded body; and laminating the magnetized molded body to produce a laminated molded body including first magnetized molded layers and second magnetized molded layers, the first magnetized molded layers and the second magnetized molded layers being alternately laminated, and a first magnetization direction of each of the first magnetized molded layers being opposite to a second magnetization direction of each of the second magnetized molded layers. 2 . The method according to claim 1 , wherein the molded body formed by extruding has a thickness of 1 mm or less. 3 . The method according to claim 1 , wherein an average particle diameter of the magnetic material is 10% or less of a thickness of the molded body. 4 . The method according to claim 1 , wherein the magnetic material comprises an Sm—Fe—N based magnetic material. 5 . The method according to claim 1 , further comprising: cutting the laminated molded body along a plane including a laminating direction of the laminated molded body to produce the bond magnet including N-poles and S-poles which are arranged alternately on a cutting face of the laminated molded body. 6 . A bond magnet comprising: a plurality of magnet pieces magnetized by axial magnetization and laminated such that N-poles and S-poles of the plurality of magnet pieces are alternately arranged, the plurality of magnet pieces comprising: an anisotropic Sm—Fe—N-based magnetic material; and a resin; and a distance λ between an N-pole among the N-poles and an S-pole adjacent to the N-pole among the S-poles is equal to or more than 0.1 mm and equal to or less than 1.0 mm. 7 . The bond magnet according to claim 6 , wherein an orientation rate of the magnetic material of the plurality of magnet pieces is 85% or more. 8 . The bond magnet according to claim 6 , wherein a magnetization rate of the plurality of magnet pieces is 95% or more. 9 . The bond magnet according to claim 6 , wherein a surface magnetic flux density B (gauss) at a position away from the bond magnet by λ/2 satisfies a following expression (1): B (gauss)>1520λ−20 (1) 10 . A method for manufacturing a bond magnet, the method comprising: providing a bond magnet composition including a magnetic material and a resin; extruding the bond magnet composition in one direction to produce a molded body; orienting the magnetic material in the one direction; magnetizing the molded body in the one direction using an axial magnetization to produce a magnetized molded body; and laminating the magnetized molded body to produce a laminated molded body including a first magnetized molded layer and a second magnetized molded layer adjacent to the first magnetized molded layer such that a first magnetization direction of the first magnetized molded layer is opposite to a second magnetization direction of the second magnetized molded layer. 11 . The method according to claim 10 , wherein extruding the bond magnet composition in the one direction while orienting the magnetic material in the one direction.
Alloys characterised by their composition · CPC title
Operations & Transport · mapped topic
Flexible forms, sheets · CPC title
Operations & Transport · mapped topic
bonded together · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.