High performance enviromentally friendly sealant composition for tire repair
US-2016289509-A1 · Oct 6, 2016 · US
US2016185053A1 · US · A1
| Field | Value |
|---|---|
| Publication number | US-2016185053-A1 |
| Application number | US-201414910802-A |
| Country | US |
| Kind code | A1 |
| Filing date | Aug 7, 2014 |
| Priority date | Aug 9, 2013 |
| Publication date | Jun 30, 2016 |
| Grant date | — |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
An object of the present invention is to provide a tire puncture sealant having excellent sealing performance and low-temperature properties. The tire puncture sealant of the present invention contains a natural rubber latex (A) and a vinyl versatate copolymer resin emulsion (B) as an emulsion of a vinyl versatate copolymer resin (b1) containing vinyl versatate as a monomer unit; the proportion of the vinyl versatate with respect to all monomer units constituting the vinyl versatate copolymer resin (b1) being from 30 to 70 mass %.
Opening claim text (preview).
1 . A tire puncture sealant containing a natural rubber latex (A) and a vinyl versatate copolymer resin emulsion (B) as an emulsion of a vinyl versatate copolymer resin (b1) containing vinyl versatate as a monomer unit; a proportion of the vinyl versatate with respect to all monomer units constituting the vinyl versatate copolymer resin (b1) being from 30 to 70 mass %. 2 . The tire puncture sealant according to claim 1 , wherein the vinyl versatate copolymer resin emulsion (B) described above contains an emulsifier (b2) containing polyvinyl alcohol; and a content of the emulsifier (b2) is from 0.8 to 3.0 mass % with respect to a solid content of the vinyl versatate copolymer resin emulsion (B). 3 . The tire puncture sealant according to claim 1 , wherein the vinyl versatate copolymer resin (b1) is an ethylene-vinyl acetate-vinyl versatate copolymer resin. 4 . The tire puncture sealant according to claim 1 , further containing a propylene glycol (C), wherein a mass ratio (B/C) of a solid content of the vinyl versatate copolymer resin emulsion (B) to the propylene glycol (C) is from 0.1 to 1.1. 5 . The tire puncture sealant according to claim 1 , wherein a mass ratio (A/B) of a solid content of the natural rubber latex (A) and a solid content of the vinyl versatate copolymer resin emulsion (B) is from 90/10 to 40/60. 6 . The tire puncture sealant according to claim 2 , wherein the vinyl versatate copolymer resin (b1) is an ethylene-vinyl acetate-vinyl versatate copolymer resin. 7 . The tire puncture sealant according to claim 2 , further containing a propylene glycol (C), wherein a mass ratio (B/C) of a solid content of the vinyl versatate copolymer resin emulsion (B) to the propylene glycol (C) is from 0.1 to 1.1. 8 . The tire puncture sealant according to claim 2 , wherein a mass ratio (A/B) of a solid content of the natural rubber latex (A) and a solid content of the vinyl versatate copolymer resin emulsion (B) is from 90/10 to 40/60. 9 . The tire puncture sealant according to claim 3 , further containing a propylene glycol (C), wherein a mass ratio (B/C) of a solid content of the vinyl versatate copolymer resin emulsion (B) to the propylene glycol (C) is from 0.1 to 1.1. 10 . The tire puncture sealant according to claim 3 , wherein a mass ratio (A/B) of a solid content of the natural rubber latex (A) and a solid content of the vinyl versatate copolymer resin emulsion (B) is from 90/10 to 40/60. 11 . The tire puncture sealant according to claim 4 , wherein a mass ratio (A/B) of a solid content of the natural rubber latex (A) and a solid content of the vinyl versatate copolymer resin emulsion (B) is from 90/10 to 40/60. 12 . The tire puncture sealant according to claim 6 , further containing a propylene glycol (C), wherein a mass ratio (B/C) of a solid content of the vinyl versatate copolymer resin emulsion (B) to the propylene glycol (C) is from 0.1 to 1.1. 13 . The tire puncture sealant according to claim 6 , wherein a mass ratio (A/B) of a solid content of the natural rubber latex (A) and a solid content of the vinyl versatate copolymer resin emulsion (B) is from 90/10 to 40/60. 14 . The tire puncture sealant according to claim 7 , wherein a mass ratio (A/B) of a solid content of the natural rubber latex (A) and a solid content of the vinyl versatate copolymer resin emulsion (B) is from 90/10 to 40/60. 15 . The tire puncture sealant according to claim 9 , wherein a mass ratio (A/B) of a solid content of the natural rubber latex (A) and a solid content of the vinyl versatate copolymer resin emulsion (B) is from 90/10 to 40/60. 16 . The tire puncture sealant according to claim 12 , wherein a mass ratio (A/B) of a solid content of the natural rubber latex (A) and a solid content of the vinyl versatate copolymer resin emulsion (B) is from 90/10 to 40/60.
Sealing compositions or agents, e.g. combined with propellant agents · CPC title
Homopolymers or copolymers of vinyl acetate · CPC title
Homopolymers or copolymers of esters of monocarboxylic acids · CPC title
Latex · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.