Crystallizer for the continuous casting of a metal product, and corresponding casting method
US-2023415223-A1 · Dec 28, 2023 · US
US12358044B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-12358044-B2 |
| Application number | US-202318243321-A |
| Country | US |
| Kind code | B2 |
| Filing date | Sep 7, 2023 |
| Priority date | Jun 28, 2019 |
| Publication date | Jul 15, 2025 |
| Grant date | Jul 15, 2025 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Continuous casting apparatus, comprising a mold and a crystallizer for the continuous casting of a metal product. The mold is provided with primary cooling means using a cooling fluid and associated with the walls of the crystallizer. A plurality of cooling members is installed downstream of the mold to perform a secondary cooling of the product, said cooling members comprising a plurality of delivery nozzles configured to deliver a liquid for cooling the product.
Opening claim text (preview).
The invention claimed is: 1. A method for continuous casting of a metal product, to obtain a productivity between 50 ton/h and 150 ton/h, the method including the following steps: supplying a continuous casting apparatus, the continuous casting apparatus comprising a mold and a crystallizer for endless, semi-endless, or billet-to-billet continuous casting of a metal product, the crystallizer having a casting cavity into which a liquid metal is cast, and the casting cavity defined by walls connected to each other in correspondence with edges, wherein an upper level of the liquid metal defines a meniscus, wherein said metal product is a billet and comprises an octagonal-shaped billet, and wherein said casting cavity has an octagonal-shaped cross-section with a distance between two opposite walls comprised between 110 mm and 220 mm and a length between 500 mm and 1500 mm; providing primary cooling means to achieve a heat exchange between the walls of the crystallizer and a skin of the metal product, with a thermal flow value in correspondence with the meniscus comprised between 6 MW/m 2 and 14 MW/m 2 and with an average value comprised between 3 MW/m 2 and 5.5 MW/m 2 ; providing a plurality of cooling members downstream of the mold to perform a secondary cooling of the cast product, wherein said cooling members comprise a plurality of delivery nozzles that deliver a liquid with a pressure at exit from said nozzles is comprised between 0.5 bar and 12 bar, and wherein specific water flow rates are between 1.2 L/kg of cast steel and 2.5 L/kg of cast steel; and casting at a casting speed between 6 m/min and 15 m/min. 2. The method as in claim 1 , wherein a pressure of a cooling fluid of the primary cooling means in a segment corresponding to an upper zone of the crystallizer, which corresponds to a vicinity of the meniscus, is comprised between 6 bar and 20 bar, and wherein the pressure of the cooling fluid of the primary cooling means in a segment corresponding to a lower zone of the crystallizer, which substantially corresponds to an end part of the crystallizer, is comprised between 2 bar and 10 bar. 3. The method as in claim 1 , further providing that said product cast product is then subjected to rolling in a rolling line in endless mode, that is, without interruptions between continuous casting and rolling. 4. The method as in claim 1 , wherein providing the plurality of cooling members downstream of the mold comprises providing a plurality of delivery nozzles that deliver the liquid with the pressure at exit from said nozzles between 1 bar and 10 bar, in which the specific water flow rates are between 1.7 L/kg of cast steel and 2.1 L/kg of cast steel. 5. The method as in claim 1 , wherein supplying the continuous casting apparatus comprises supplying foot rolls, disposed at an exit of the crystallizer, for a guide length comprised between 150 mm and 800 mm, in which the cast product at exit from said mold follows a casting line with an aid of a plurality of guide rolls disposed directly downstream of said foot rolls following a machine radius comprised between 5 m and 25 m. 6. The method as in claim 1 , wherein providing the primary cooling means comprises providing a cooling fluid of said primary cooling means a distance from the walls of the crystallizer in contact with the liquid metal, the distance comprised between 8 mm and 10 mm. 7. The method as in claim 1 , wherein providing the primary cooling means comprises providing a pressure of a cooling fluid of the primary cooling means in a vicinity of the meniscus is comprised between 6 bar and 20 bar, and in which the pressure of the cooling fluid of the primary cooling means in a zone corresponding to an end part of the crystallizer is comprised between 2 bar and 10 bar. 8. The method as in claim 1 , wherein the primary cooling means is configured to exchange thermal flows comprised between 6 MW/m 2 and 10 MW/m 2 .
for curved casting · CPC title
for plastic shaping of strands (rolling mills B21B1/46) · CPC title
Feeding additives, powders, or the like · CPC title
Lubricating the moulds · CPC title
Mould materials or platings · CPC title