Continuous casting mold and method for continuous casting of steel
US-2015258603-A1 · Sep 17, 2015 · US
US11020794B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-11020794-B2 |
| Application number | US-201716342576-A |
| Country | US |
| Kind code | B2 |
| Filing date | Oct 16, 2017 |
| Priority date | Oct 19, 2016 |
| Publication date | Jun 1, 2021 |
| Grant date | Jun 1, 2021 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A continuous casting mold including a water-cooled copper mold having a mold copper plate including an inner wall surface, recessed portions disposed partially or entirely in a region of the inner wall surface of the water-cooled copper mold from at least a position located at a meniscus to a position located 20 mm lower than the meniscus, and material-filled layers disposed in the recessed portions with a metal or nonmetal having a thermal conductivity different from that of the mold copper plate of the water-cooled copper mold. A shape of each of the recessed portions at a surface of the mold copper plate includes a curved surface.
Opening claim text (preview).
The invention claimed is: 1. A continuous casting mold comprising: a water-cooled copper mold having a mold copper plate including an inner wall surface; recessed portions disposed partially or entirely in a region of the inner wall surface of the water-cooled copper mold from at least a position located at a meniscus to a position located 20 mm lower than the meniscus; and material-filled layers disposed in the recessed portions with a metal or nonmetal having a thermal conductivity different from that of the mold copper plate of the water-cooled copper mold, wherein a shape of each of the recessed portions at a surface of the mold copper plate includes a curved surface having a curvature in every direction and a flat surface, and the curved surface has a radius of curvature satisfying the formula (1) below: d/ 2< R≤d (1) where d is a minimum opening width (mm) of the recessed portions at the inner wall surface of the mold copper plate, and R is an average radius of curvature (mm) of the recessed portions. 2. The continuous casting mold according to claim 1 , wherein the radius of curvature is a constant value. 3. A method for continuously casting steel, the method comprising: providing the continuous casting mold according to claim 2 ; pouring molten steel in a tundish into the continuous casting mold; and continuously casting the molten steel. 4. The continuous casting mold according to claim 1 , wherein an opening shape of one recessed portion at the inner wall surface of the mold copper plate is elliptic, and all adjacent recessed portions are not in contact with or connected to one another. 5. A method for continuously casting steel, the method comprising: providing the continuous casting mold according to claim 4 ; pouring molten steel in a tundish into the continuous casting mold; and continuously casting the molten steel. 6. The continuous casting mold according to claim 1 , wherein an opening shape of one recessed portion at the inner wall surface of the mold copper plate is elliptic, and all or some adjacent recessed portions are in contact with or connected to one another. 7. A method for continuously casting steel, the method comprising: providing the continuous casting mold according to claim 6 ; pouring molten steel in a tundish into the continuous casting mold; and continuously casting the molten steel. 8. The continuous casting mold according to claim 1 , wherein an opening shape of one recessed portion at the inner wall surface of the mold copper plate is circular, and all adjacent recessed portions are not in contact with or connected to one another. 9. A method for continuously casting steel, the method comprising: providing the continuous casting mold according to claim 8 ; pouring molten steel in a tundish into the continuous casting mold; and continuously casting the molten steel. 10. The continuous casting mold according to claim 1 , wherein an opening shape of one recessed portion at the inner wall surface of the mold copper plate is circular, and all or some adjacent recessed portions are in contact with or connected to one another. 11. A method for continuously casting steel, the method comprising: providing the continuous casting mold according to claim 10 ; pouring molten steel in a tundish into the continuous casting mold; and continuously casting the molten steel. 12. A method for continuously casting steel, the method comprising: providing the continuous casting mold according to claim 1 ; pouring molten steel in a tundish into the continuous casting mold; and continuously casting the molten steel. 13. A continuous casting mold comprising: a water-cooled copper mold having a mold copper plate including an inner wall surface; recessed portions disposed partially or entirely in a region of the inner wall surface of the water-cooled copper mold from at least a position located at a meniscus to a position located 20 mm lower than the meniscus; and material-filled layers disposed in the recessed portions with a metal or nonmetal having a thermal conductivity different from that of the mold copper plate of the water-cooled copper mold, wherein a shape of each of the recessed portions at a surface of the mold copper plate, at any position of the recessed portion, is a curved surface having a curvature in every direction, and the curved surface has a radius of curvature satisfying the formula (1) below: d/ 2< R≤d (1) where d is a minimum opening width (mm) of the recessed portions at the inner wall surface of the mold copper plate, and R is an average radius of curvature (mm) of the recessed portions. 14. The continuous casting mold according to claim 13 , wherein the radius of curvature is a constant value. 15. A method for continuously casting steel, the method comprising: providing the continuous casting mold according to claim 14 ; pouring molten steel in a tundish into the continuous casting mold; and continuously casting the molten steel. 16. A method for continuously casting steel, the method comprising: providing the continuous casting mold according to claim 13 ; pouring molten steel in a tundish into the continuous casting mold; and continuously casting the molten steel.
Controlling or regulating processes or operations · CPC title
Mould materials or platings · CPC title
Moulds with special profile · CPC title
into open-ended moulds (B22D11/06, B22D11/07 take precedence; plants for continuous casting, e.g. for upwardly drawing the strand B22D11/14) · CPC title
for cooling cast stock or mould · CPC title