Binder composition for non-aqueous secondary battery functional layer, slurry composition for non-aqueous secondary battery functional layer, non-aqueous secondary battery member, and non-aqueous secondary battery
US-11831019-B2 · Nov 28, 2023 · US
US12355059B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-12355059-B2 |
| Application number | US-201917288396-A |
| Country | US |
| Kind code | B2 |
| Filing date | Oct 18, 2019 |
| Priority date | Oct 26, 2018 |
| Publication date | Jul 8, 2025 |
| Grant date | Jul 8, 2025 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
The present invention provides a method of preparing an electrode for a lithium secondary battery which includes forming a first electrolyte layer by immersing an electrode current collector in a composition for forming the first electrolyte layer and applying a current, and forming a second electrolyte layer by immersing the electrode current collector having the first electrolyte layer formed thereon in a composition for forming the second electrolyte layer and applying a current, wherein one of the composition for forming the first electrolyte layer and the composition for forming the second electrolyte layer is a composition for forming an organic electrolyte layer, and another one is a composition for forming an inorganic electrolyte layer, and the composition for forming an inorganic electrolyte layer includes a compound represented by Formula 1.
Opening claim text (preview).
The invention claimed is: 1. A method of preparing a positive electrode for a lithium secondary battery, comprising: forming an inorganic electrolyte layer directly on a positive electrode current collector by immersing the positive electrode current collector in a composition for forming the inorganic electrolyte layer and applying a current; and forming an organic electrolyte layer by immersing the positive electrode current collector having the inorganic electrolyte layer formed thereon in a composition for forming the organic electrolyte layer and applying a current, wherein the composition for forming the inorganic electrolyte layer comprises a compound represented by Formula 1: MM′X n- m(SO 2 ) [Formula 1] M is a metallic element selected from the group consisting of lithium (Li), sodium (Na), potassium (K), and rubidium (Rb), M′ is a metallic element selected from the group consisting of aluminum (Al), gallium (Ga), indium (In), and titanium (Ti), X is a halogen element selected from the group consisting of fluorine (F), chlorine (Cl), bromine (Br), and iodine (I), n is an integer of 1 to 6, and m is an integer of 1 to 10, the composition for forming the organic electrolyte layer comprises an organic solvent and a lithium salt, and the lithium salt includes Li + as a cation and at least one selected from the group consisting of F − , Cl − , Br − , I − , NO 3 − , BF 4 − , ClO 4 − , AlO 4 − , AlCl 4 − , PF 6 − , SbF 6 − , AsF 6 − , BF 2 C 2 O 4 − , BC 4 O 8 − , (CF 3 ) 2 PF 4 − , (CF 3 ) 3 PF 3 − , (CF 3 ) 4 PF 2 − , (CF 3 ) 5 PF − , (CF 3 ) 6 P − , CF 3 SO 3 − , C 4 F 9 SO 3 − , CF 3 CF 2 SO 3 − , CF 3 CF 2 (CF 3 ) 2 CO, (CF 3 SO 2 ) 2 CH, CF 3 (CF 2 ) 7 SO 3 − , CF 3 CO 2 − , CH 3 CO 2 − , SCN − , and mixture thereof. 2. The method of claim 1 , wherein the organic solvent comprises at least one compound selected from the group consisting of a halogen element-substituted or unsubstituted carbonate-based compound, a halogen element-substituted or unsubstituted acetate-based compound, a halogen element-substituted or unsubstituted glyme-based compound, a halogen element-substituted or unsubstituted ether-based compound, and a halogen element-substituted or unsubstituted nitrile-based compound. 3. The method of claim 1 , wherein the composition for forming the organic electrolyte layer further comprises an additive, wherein the additive comprises at least one compound selected from the group consisting of vinylene carbonate, vinylethylene carbonate, propanesultone, propenesultone, lithium difluoro (oxalato) phosphate, lithium difluoro (oxalato) borate, lithium tetrafluorooxalate phosphate, succinonitrile, succinic anhydride, ethylene sulfate, ethylene glycol bis (propionitrile) ether, lithium tetrafluoroborate, fluoroethylene carbonate, and lithium difluorophosphate. 4. The method of claim 1 , wherein the compound represented by Formula 1 comprises at least one compound selected from the group consisting of LiAlCl 4 -3(SO 2 ) and NaAlCl 4 -2(SO 2 ). 5. The method of claim 1 , wherein the composition for forming an inorganic electrolyte layer further comprises an inorganic ionic liquid. 6. A positive electrode for a lithium secondary battery, comprising a positive electrode current collector, an inorganic electrolyte layer and an organic electrolyte layer sequentially disposed in an order listed on the positive electrode current collector, wherein the inorganic electrolyte layer comprises a reduced compound of a compound represented by Formula 1: MM′Xn-m(SO2) [Formula 1] M is a metallic element selected from the group consisting of lithium (Li), sodium (Na), potassium (K), and rubidium (Rb), M′ is a metallic element selected from the group consisting of aluminum (Al), gallium (Ga), indium (In), and titanium (Ti), X is a halogen element selected from the group consisting of fluorine (F), chlorine (Cl), bromine (Br), and iodine (I), n is an integer of 1 to 6, and m is an integer of 1 to 10, wherein the organic electrolyte layer or the inorganic electrolyte layer is disposed on the positive electrode current collector. 7. The positive electrode for a lithium secondary battery of claim 6 , wherein the organic electrolyte layer and the inorganic electrolyte layer are mixed and present in one layer. 8. The method of claim 1 , wherein the current for forming the inorganic electrolyte is in a range of −1 V to 5.0 V from an open circuit voltage (OCV). 9. The method of claim 1 , wherein the current for forming the inorganic electrolyte is in a range of −0.2 V to 4.5 V from an open circuit voltage (OCV). 10. The method of claim 1 , wherein the current for forming the inorganic electrolyte is in a range of −0.2 V to 4.5 V from an open circuit voltage (OCV). 11. The electrode for a lithium secondary battery of claim 6 , wherein a current in a range of −1 V to 5.0 V from an open circuit voltage (OCV) is applied for forming the inorganic electrolyte layer. 12. The electrode for a lithium secondary battery of claim 6 , wherein a current in a range of −0.2 V to 4.5 V from an open circuit voltage (OCV) is applied for forming the inorganic electrolyte layer. 13. The electrode for a lithium secondary battery of claim 6 , wherein a current in a range of −0.2 V to 4.5 V from an open circuit voltage (OCV) is applied for forming the inorganic electrolyte layer. 14. The method of claim 1 , wherein the composition for forming an organic electrolyte layer comprises cyclic carbonate-based compound or linear carbonate-based compound. 15. The method of claim 1 , wherein the composition for forming the organic electrolyte layer comprises at least one selected from the group consisting of ethylene carbonate, propylene carbonate, 1,2-butylene carbonate, 2,3-butylene carbonate, 1,2-pentylene carbonate, 2,3-pentylene carbonate, vinylene carbonate, and fluoroethyelen carbonate. 16. The method of claim 1 , wherein the composition for forming the inorganic electrolyte layer comprises LiAlCl 4 -3(SO 2 ). 17. The method of claim 1 , wherein the composition for forming the inorganic electrolyte layer comprises NaAlCl 4 -2(SO 2 ). 18. The method of claim 1 , wherein a concentration of the lithium salt in the composition for forming the organic electrolyte layer is 1.0 M to 3.0 M.
Halides · CPC title
Chlorides · CPC title
Carbonates · CPC title
characterised by the solvent · CPC title
characterised by the solvents · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.