Positive electrode for lithium ion battery
US-2020168896-A1 · May 28, 2020 · US
US12046749B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-12046749-B2 |
| Application number | US-202117463912-A |
| Country | US |
| Kind code | B2 |
| Filing date | Sep 1, 2021 |
| Priority date | Nov 28, 2018 |
| Publication date | Jul 23, 2024 |
| Grant date | Jul 23, 2024 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Provided is a lithium secondary battery with improved t electrochemical characteristics through improvement of the structural stability by including a cathode active material doped with molybdenum (Mo). The lithium secondary battery includes a cathode; an anode; a separator positioned between the cathode and the anode; and an electrolyte. In particular, the cathode active material includes molybdenum (Mo) doped on a composite oxide of lithium and metal including manganese (Mn) and titanium (Ti).
Opening claim text (preview).
What is claimed is: 1. A method of manufacturing a cathode active material, comprising: performing milling on metal oxides; drying the milled metal oxides; and performing heat treatment on the dried metal oxides to obtain a cathode active material, wherein the metal oxides comprise oxides of lithium (Li), manganese (Mn), titanium (Ti) and molybdenum (Mo), and wherein the cathode active material comprises a composite having the following formula, Li 1.2 [(Mn 0.4 Ti 0.4 ) 0.95 Mo 0.05 ]O 2 . 2. The method of claim 1 , wherein the milling is performed by ball milling. 3. The method of claim 2 , wherein the ball milling is repeated two or more times each for about 15 minutes at a rotation speed of about 300 rpm. 4. The method of claim 3 , wherein the ball milling is repeated 17 times. 5. The method of claim 1 , wherein the heat treatment is performed in an argon (Ar) atmosphere at a temperature of about 900° C. for about 12 hours.
Energy storage using batteries · CPC title
of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx · CPC title
of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence) · CPC title
Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx · CPC title
characterised by the use of electrical cells or batteries (for propulsion puposes B60K1/04; supplying batteries to, or removing batteries from, vehicles B60S5/06; testing of charge state G01R31/36) · CPC title