Water-developable photosensitive resin composition for flexographic printing and photosensitive resin original plate for flexographic printing obtained therefrom

US11656551B2 · US · B2

Patent metadata
FieldValue
Publication numberUS-11656551-B2
Application numberUS-201816644343-A
CountryUS
Kind codeB2
Filing dateAug 31, 2018
Priority dateSep 5, 2017
Publication dateMay 23, 2023
Grant dateMay 23, 2023

How to read this patent

A practical reading order for non-experts. Skip the full description unless you need deep technical detail.

  1. Title

    What the patent document calls the invention.

  2. Abstract

    A short plain-language summary of the technical disclosure.

  3. Assignees and inventors

    Who owns or filed the patent and who is credited as inventor.

  4. Key dates

    Filing, priority, publication, and grant dates set the timeline.

  5. First independent claim

    The legal scope of protection — read this for what is actually claimed.

  6. CPC / IPC classifications

    Technology tags used to group this patent with similar filings.

  7. Citations and related patents

    Prior art links and similar publications in this corpus.

Abstract

Official abstract text for this publication.

A photosensitive resin composition for a flexographic printing original plate is disclosed which exhibits reduced adhesion of dust, dirt, and paper powder, resistance to UV ink and allows storage of the printing original plate for a long period of time. A water-developable photosensitive resin composition for flexographic printing, contains at least a polyamide and/or a polyamide block copolymer (a), a cross-linking agent having one or more unsaturated group(s) (b), a photo-polymerization initiator (c), and a fatty acid ester (d), wherein the fatty acid ester (d) has two or more hydroxyl groups and 24 or 25 carbon atoms in a molecule, wherein the fatty acid ester (d) is a fatty acid ester of a compound selected from fatty acids having a number of carbon atoms of 12 to 22, and wherein a content of the fatty acid ester (d) in the photosensitive resin composition is 0.2 to 6% by weight.

First claim

Opening claim text (preview).

The invention claimed is: 1. A water-developable photosensitive resin composition for flexographic printing, comprising at least a polyamide and/or a polyamide block copolymer (a), a cross-linking agent having one or more unsaturated group(s) (b), a photo-polymerization initiator (c), and a fatty acid ester (d), wherein the fatty acid ester (d) has two or more hydroxyl groups and 24 or 25 carbon atoms in a molecule, wherein the fatty acid ester (d) is a fatty acid ester of a compound selected from fatty acids having a number of carbon atoms of 12 to 22, and wherein a content of the fatty acid ester (d) in the photosensitive resin composition is 0.2 to 6% by weight, and wherein the water-developable photosensitive resin composition does not contain rubber component. 2. The water-developable photosensitive resin composition for flexographic printing according to claim 1 , wherein the photosensitive resin composition contains 40 to 60% by weight of the polyamide and/or the polyamide block copolymer (a), 20 to 50% by weight of the cross-linking agent having one or more unsaturated group(s) (b), and 0.1 to 10% by weight of the photo-polymerization initiator (c), and wherein the polyamide and/or the polyamide block copolymer (a) contain(s), in a molecule, 50% by weight or more of a structural unit constituted from an amide bond in a block form. 3. The water-developable photosensitive resin composition for flexographic printing according to claim 1 , wherein the fatty acid ester (d) is sorbitan monooleate, sorbitan monostearate or glycerol monobehenate. 4. A photosensitive resin original plate for flexographic printing, comprising a photosensitive resin layer constituted from the water-developable photosensitive resin composition for flexographic printing according to claim 1 , a support and an adhesive layer for adhering them. 5. The photosensitive resin original plate for flexographic printing according to claim 4 , in combination with a UV ink or a UV varnish. 6. The water-developable photosensitive resin composition for flexographic printing according to claim 1 , wherein the content of the fatty acid ester (d) in the photosensitive resin composition is 4 to 6% by weight.

Assignees

Inventors

Classifications

  • having cover layers or intermediate layers, e.g. subbing layers {(G03F7/091 - G03F7/093, B41N3/03 take precedence)} · CPC title

  • G03F7/037Primary

    the binders being polyamides or polyimides · CPC title

  • Lactams · CPC title

  • non-metallic other than stone {, e.g. printing plates or foils comprising inorganic materials in an organic matrix (B41N1/003, B41N1/006 take precedence)} · CPC title

Patent family

Related publications grouped by family.

External sources

Frequently asked questions

Answers are generated from the same data shown on this page.

What does patent US11656551B2 cover?
A photosensitive resin composition for a flexographic printing original plate is disclosed which exhibits reduced adhesion of dust, dirt, and paper powder, resistance to UV ink and allows storage of the printing original plate for a long period of time. A water-developable photosensitive resin composition for flexographic printing, contains at least a polyamide and/or a polyamide block copolyme…
Who is the assignee on this patent?
Toyo Boseki
What technology area does this patent fall under?
Primary CPC classification G03F7/037. Mapped technology areas include Physics.
When was this patent published?
Publication date Tue May 23 2023 00:00:00 GMT+0000 (Coordinated Universal Time) (B2). Legal status and post-grant events are not shown on this page.
What related patents are in patentsdb?
We list 8 related publications on this page (citations in our corpus or others sharing the same primary CPC).