Borosilicate glass for pharmaceutical container and glass tube for pharmaceutical container
US-10099956-B2 · Oct 16, 2018 · US
US11542191B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-11542191-B2 |
| Application number | US-201816648878-A |
| Country | US |
| Kind code | B2 |
| Filing date | Oct 16, 2018 |
| Priority date | Oct 20, 2017 |
| Publication date | Jan 3, 2023 |
| Grant date | Jan 3, 2023 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
The present invention relates to a glass for a pharmaceutical container that is excellent in ultraviolet shielding ability, and is also excellent in chemical durability. The glass for a pharmaceutical container of the present invention includes as a glass composition, in terms of mass %, 67% to 81% of SiO2, more than 4% to 7% of Al2O3, 7% to 14% of B2O3, 3% to 12% of Na2O+K2O, 0% to 1.8% of CaO+BaO, 0.5% to less than 2% of Fe2O3, and 1% to 5% of TiO2, and satisfies a relationship of CaO/BaO≤0.5.
Opening claim text (preview).
The invention claimed is: 1. A glass for a pharmaceutical container, which comprises as a glass composition, in terms of mass %, 67% to 81% of SiO 2 , more than 4% to 7% of Al 2 O 3 , 7% to 14% of B 2 O 3 , 6% to 8.55% of Na 2 O+K 2 O, 0.8% to 1.8% of CaO+BaO, 0.1% to 1.8% of BaO, 0.5% to less than 2% of Fe 2 O 3 , and 1% to 5% of TiO 2 , and satisfies a relationship of CaO/BaO≤0.4, wherein the glass has a transmittance at a wavelength of 450 nm that is 15% or less when having a thickness of 1 mm. 2. The glass for a pharmaceutical container according to claim 1 , wherein the glass comprises as a glass composition, in terms of mass %, 70% to 78% of SiO 2 , 5% to 7% of Al 2 O 3 , 8% to 11% of B 2 O 3 , 6% to 8.55% of Na 2 O+K 2 O, 0.8% to 1.8% of CaO+BaO, 0.8% to 1.2% of Fe 2 O 3 , and 2% to 5% of TiO 2 , and satisfies a relationship of CaO/BaO≤0.3. 3. The glass for a pharmaceutical container according to claim 2 , wherein the glass comprises as a glass composition, in terms of mass %, 9% to 11% of B2O 3 . 4. The glass for a pharmaceutical container according to claim 1 , wherein the glass comprises as a glass composition, in terms of mass %, 9% to 11% of B 2 O 3 . 5. The glass for a pharmaceutical container according to claim 1 , wherein the glass has a consumption amount of 0.02 mol/L hydrochloric acid per unit glass mass 0.035 mL or less in a hydrolytic resistance test by a glass grains test method in conformity with the European Pharmacopoeia 7.0. 6. The glass for a pharmaceutical container according to claim 1 , wherein the glass has a working point of 1,200° C. or less. 7. A glass tube for a pharmaceutical container, comprising the glass for a pharmaceutical container of claim 1 . 8. A glass tube for a pharmaceutical container, comprising the glass for a pharmaceutical container of claim 2 . 9. A glass tube for a pharmaceutical container, comprising the glass for a pharmaceutical container of claim 4 . 10. A glass tube for a pharmaceutical container, comprising the glass for a pharmaceutical container of claim 5 . 11. A glass tube for a pharmaceutical container, comprising the glass for a pharmaceutical container of claim 6 . 12. A glass tube for a pharmaceutical container, comprising the glass for a pharmaceutical container of claim 3 . 13. A glass for a container, which comprises as a glass composition, in terms of mass %, 67% to 81% of SiO 2 , more than 4% to 7% of Al 2 O 3 , 7% to 14% of B 2 O 3 , 6% to 8.55% of Na 2 O+K 2 O, 0.8% to 1.8% of CaO+BaO, 0.1% to 1.8% of BaO, 0.5% to less than 2% of Fe 2 O 3 , and 1% to 5% of TiO 2 , and satisfies a relationship of CaO/BaO≤0.4, wherein the glass has a transmittance at a wavelength of 450 nm that is 15% or less when having a thickness of 1 mm. 14. A glass tube for a container, comprising the glass for a container of claim 13 .