A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A process for treating wood strands suitable for producing OSBs includes treating the wood strands in water at a temperature in the range from 50° C. to 100° C. The present invention likewise relates to a process for producing wood-based OSBs, in particular wood-based OSBs having reduced emission of volatile organic compounds (VOCs), including: a) production of wood strands from suitable timbers; b) treatment of at least part of the wood strands with water; c) drying of the wood strands which have been treated with the water; d) coating of the wood strands which have been treated with water and dried and coating of wood strands which have not been treated with water with at least one binder; e) scattering of the glue-coated wood strands on a conveyor belt; and f) pressing of the glue-coated wood strands to give a wood-based OSB.
Opening claim text (preview).
The invention claimed is: 1. A process for producing wood-based OSBs comprising: a) production of wood strands from suitable timbers; b) treatment of at least part of the wood strands with water having a temperature in the range from 50° C. to 100° C. for a time of from 10 to 60 minutes; c) drying of the wood strands which have been treated in the water; d) coating of the wood strands which have been treated with water and dried and optionally coating of wood strands which have not been treated with water with at least one binder; e) scattering of the binder-coated wood strands on a conveyor belt; and f) pressing of the binder-coated wood strands to give a wood-based OSB. 2. The process according to claim 1 , wherein water-treated wood strands or a mixture of water-treated wood strands and wood strands which have not been treated with water are used as middle layer and/or covering layer of the wood-based OSB. 3. The process according to claim 1 , wherein the step of treatment of the wood strands with water is carried out separately from the production process for the OSBs or is integrated into the production process for the OSBs. 4. The process according to claim 1 , wherein the wood strands which have been treated with water and have not been treated with water are coated with an amount of binder of from 1.0 to 5.0% by weight based on the total amount of the wood strands. 5. The process according to claim 1 , wherein the binder-coated wood strands are pressed at temperatures in the range from 200 to 250° C. to give the wood-based OSB. 6. The process according to claim 1 , wherein the wood strands which have been treated with water and have not been treated with water are coated with an amount of binder of from 2 to 4% by weight based on the total amount of the wood strands. 7. The process according to claim 1 , wherein the binder-coated wood strands are pressed at temperatures in the range from 220 to 230° C. to give the wood-based OSB. 8. The process according to claim 1 , wherein treatment of the wood strands are treated with water having a temperature in the range from 60 to 90° C. 9. The process according to claim 1 , wherein treatment of the wood strands are treated with water having a temperature in the range from 70 to 90° C. 10. The process according to claim 1 , wherein the treatment of the wood strands with water is carried out for a time of from 15 to 45 minutes. 11. The process according to claim 1 , wherein the treatment of the wood strands with water is carried out for a time of from 20 to 30 minutes. 12. The process according to claim 1 , wherein the wood strands are covered completely by water during the treatment. 13. The process according to claim 12 , wherein the wood strands are completely immersed in the water. 14. The process according to claim 1 , wherein the wood strands are conveyed continuously on at least one transport device through an apparatus containing the water for the water treatment. 15. The process according to claim 14 , comprising discharging the water from the apparatus after passage of the wood strands. 16. The process according to claim 15 , comprising purifying the water discharged from the apparatus and recirculating the purified water into the apparatus.
Damping wood · CPC title
of solids · CPC title
Extraction of components naturally occurring in wood, cork, straw, cane or reed · CPC title
Apparatus · CPC title