Method for producing vinyl ether polymer having hydroxyl group on side chain and temperature-responsive polymer mixture
US-2018371127-A1 · Dec 27, 2018 · US
US10633469B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10633469-B2 |
| Application number | US-201615579301-A |
| Country | US |
| Kind code | B2 |
| Filing date | Jun 29, 2016 |
| Priority date | Jul 3, 2015 |
| Publication date | Apr 28, 2020 |
| Grant date | Apr 28, 2020 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A method for producing a hydroxyl group-containing vinyl ether polymer according to the present invention includes: a step of radical polymerizing at least one vinyl ether selected from vinyl ether having a hydroxyl group represented by the following formula (2): wherein R 7 represents an alkylene group which is straight-chained, branched or comprises an alicyclic structure, and p is 1, 2, or 3, in the presence of water as a polymerization solvent and an azo compound represented by the following formula (1) as a polymerization initiator: wherein R 1 to R 4 each independently represent a hydrogen atom or an alkyl group and R 5 and R 6 each independently represent an alkoxy group optionally having a substituent group or an alkyl amino group optionally having a substituent group.
Opening claim text (preview).
The invention claimed is: 1. A method for producing a hydroxyl group-containing vinyl ether polymer, comprising: a step of radical polymerizing at least one vinyl ether selected from vinyl ether having a hydroxyl group represented by the following formula (2): wherein R 7 represents an alkylene group which is straight-chained, branched or comprises an alicyclic structure, and p is 1, 2, or 3, in the presence of water as a polymerization solvent and dimethyl 2,2′-azobis (2- methylpropionate) as a polymerization initiator, and the amount of said dimethyl 2,2′-azobis (2-methylpropionate) added is from 0.01 to 0.5 mol % based on said vinyl ether, wherein the monomer conversion rate is 95% or more in the step of radical polymerization. 2. The method for producing a polymer according to claim 1 , wherein the monomer conversion rate is 99% or more in the step of radical polymerization. 3. The method for producing a polymer according to claim 1 , wherein the amount of said dimethyl 2,2′-azobis(2-methylpropionate) added is from 0.01 to 0.2 mol % based on said vinyl ether and the number average molecular weight Mn of the hydroxyl group-containing vinyl ether polymer is from 10,000 to 600,000. 4. A method for producing an aqueous hydroxyl group-containing vinyl ether polymer solution comprising water and a hydroxyl group-containing vinyl ether polymer, the method comprising: a step of radical polymerizing at least one vinyl ether selected from vinyl ether having a hydroxyl group represented by the following formula (2): wherein R 7 represents an alkylene group which is straight-chained, branched or comprises an alicyclic structure, and p is 1, 2, or 3, in the presence of water as a polymerization solvent and dimethyl 2,2′-azobis(2-methylpropionate) as a polymerization initiator, and the amount of said dimethyl 2 2′-azobis (2-methylpropionate) added is from 0.01 to 0.5 mol % based on said vinyl ether, wherein the monomer conversion rate is 95% or more in the step of radical polymerization; and a step of storing the obtained hydroxyl group-containing vinyl ether polymer in an aqueous solution. 5. The method for producing an aqueous polymer solution according to claim 4 , wherein the monomer conversion rate is 99% or more in the step of radical polymerization. 6. The method for producing an aqueous polymer solution according to claim 4 , wherein the amount of said dimethyl 2,2′-azobis(2-methylpropionate) added is from 0.01 to 0.2 mol % based on said vinyl ether and the number average molecular weight Mn of the hydroxyl group-containing vinyl ether polymer is from 10,000 to 600,000.
Acyclic compounds · CPC title
Azo-compounds · CPC title
Monomers containing only one unsaturated aliphatic radical · CPC title
Homopolymers or copolymers of unsaturated ethers (C08L35/08 takes precedence) · CPC title
Homopolymers or copolymers of unsaturated ethers (C09D135/08 takes precedence) · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.