Carbon fiber reinforcements for sheet molding composites
US-9815224-B2 · Nov 14, 2017 · US
US10486338B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10486338-B2 |
| Application number | US-201615559275-A |
| Country | US |
| Kind code | B2 |
| Filing date | Mar 2, 2016 |
| Priority date | Mar 19, 2015 |
| Publication date | Nov 26, 2019 |
| Grant date | Nov 26, 2019 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A process for producing a resin-impregnated fiber bundle includes an unwinding step in which a resin-unimpregnated fiber bundle is unwound, a resin impregnation step in which the fiber bundle is passed through an impregnation bath filled with a resin, and an impregnation acceleration step in which after the resin impregnation step, the resin is permeated into the fiber bundle, at least the impregnation acceleration step being performed in a decompression space having a pressure lower than atmospheric pressure. It is possible to produce a resin-impregnated fiber bundle using a decompression space for which decompression can be achieved with a simple device and in which the airtightness is easy to maintain and which has been configured so as to result in satisfactory working efficiency.
Opening claim text (preview).
The invention claimed is: 1. A process for producing a resin-impregnated fiber bundle by continuously impregnating with a resin a fiber bundle continuously travelling, comprising: an unwinding step in which a resin-unimpregnated fiber bundle is unwound; a resin impregnation step in which the fiber bundle is passed into an impregnation bath filled with a resin; and an impregnation acceleration step in which the resin is permeated into the fiber bundle after the resin impregnation step, wherein at least the impregnation acceleration step is performed in a decompression space having a pressure lower than atmospheric pressure, the decompression space comprises two or more partition walls sectioned in a direction approximately orthogonal to a travelling direction of the fiber bundle and has a pressure lower than a pressure in a space to perform the unwinding step and/or the resin impregnation step, and an airtight wall structure having a fiber bundle pass-through for the fiber bundle to pass through is provided in the decompression space, wherein one or more vacuum suction ports are provided in the airtight wall structure while one or more additional vacuum suction ports are further provided outside the airtight wall structure, the one or more vacuum suction ports and one or more additional vacuum suction ports being provided on at least one of the two or more partition walls. 2. The process according to claim 1 , wherein the decompression space is a vacuum. 3. The process according to claim 1 , wherein an outer surface of the two or more partition walls is provided with a fiber bundle pass-through to supply and/or discharge the fiber bundle. 4. The process according to claim 1 , wherein a fiber bundle pass-through provided on an outer surface of one of the two or more partition walls has an opening area equal to or less than an opening area of the fiber bundle pass-through in the airtight wall structure. 5. The process according to claim 4 , wherein one or more fiber bundle pass-throughs are provided on at least one of the two or more partition walls, and the fiber bundle pass-throughs on the two or more partition walls or the airtight wall structure are not on a plane formed as including the travelling direction of the fiber bundle and a width direction of the fiber bundle pass-through at the most upstream fiber bundle pass-through. 6. The process according to claim 1 , wherein a tip of an airtight wall forming the fiber bundle pass-through in the airtight wall structure is formed in a fiber bundle guide shape to lead the fiber bundle downstream by contacting the fiber bundle. 7. The process according to claim 1 , wherein the fiber bundle pass-through is quadrangular. 8. The process according to claim 1 , wherein a sheet type elastic member that maintains airtightness is sandwiched on a contact surface between the two or more partition walls in the decompression space. 9. The process according to claim 8 , wherein the fiber bundle pass-through is formed with the sheet type elastic member, two or more partition walls and an airtight wall in the decompression space. 10. The process according to claim 1 , wherein two or more additional yarn guide members sectioned in the direction approximately orthogonal to the travelling direction of the fiber bundle are sandwiched with the two or more partition walls and an airtight wall to form the fiber bundle pass-through in the decompression space. 11. The process according to claim 1 , wherein the impregnation acceleration step comprises a step of passing the fiber bundle onto an impregnation acceleration bar that is prevented from rotating. 12. The process according to claim 1 , wherein the impregnated fiber bundle is wound with a freely movable winding head onto a mandrel rotating around a fixed shaft to make a roll product after passing through the impregnation acceleration step. 13. A process of producing a resin-impregnated fiber bundle by continuously impregnating with a resin a fiber bundle continuously travelling, comprising: an unwinding step in which a resin-unimpregnated fiber bundle is unwound; a resin impregnation step in which the fiber bundle is passed into an impregnation bath filled with a resin; and an impregnation acceleration step in which the resin is permeated into the fiber bundle after the resin impregnation step, wherein at least the impregnation acceleration step is performed in a decompression space having a pressure lower than atmospheric pressure, the decompression space comprises two or more partition walls sectioned in a direction approximately orthogonal to a travelling direction of the fiber bundle and has a pressure lower than a pressure in a space to perform the unwinding step and/or the resin impregnation step, an airtight wall structure having a fiber bundle pass-through for the fiber bundle to pass through is provided in the decompression space, and one or more fiber bundle pass-throughs are provided on at least one of the two or more partition walls; wherein one or more of the fiber bundle pass-throughs provided on the two or more partition walls or the airtight wall structure are not on a plane formed as including the travelling direction of the fiber bundle and a width direction of the fiber bundle pass-through at a most upstream fiber bundle pass-through.
by mechanical means · CPC title
by dipping · CPC title
Unwinding, paying-out webs {(reel-to-reel type web winding and unwinding mechanisms B65H18/103, B65H18/145)} · CPC title
Web-winding mechanisms · CPC title
performed by dipping · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.