Ysz ceramic substrate protected fireproof hose
US-2024401725-A1 · Dec 5, 2024 · US
US10280869B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10280869-B2 |
| Application number | US-201414901273-A |
| Country | US |
| Kind code | B2 |
| Filing date | Jan 24, 2014 |
| Priority date | Jun 25, 2013 |
| Publication date | May 7, 2019 |
| Grant date | May 7, 2019 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A rubber-metal laminated gasket material comprising a metal plate, a surface treating agent layer, an adhesive layer, and a rubber layer, the layers being sequentially laminated on the metal plate; wherein the surface treating agent layer is formed by applying a surface treating agent so that the coating amount on one surface is 30 to 1,000 mg/m2, and the surface treating agent is free from chromium, has a mixing ratio of 20 to 90 wt. % of a fluorine-free titanium compound and 10 to 80 wt. % of alumina, and has a metal titanium content of 1 to 20 wt. %. The rubber-metal laminated gasket material has excellent LLC resistance under high temperature conditions.
Opening claim text (preview).
The invention claimed is: 1. A rubber-metal laminated gasket material comprising a metal plate, a surface treating agent layer, an adhesive layer, and a rubber layer, the layers being sequentially laminated on the metal plate in the recited order; wherein the surface treating agent layer is formed by applying a surface treating agent so that the coating amount on one surface is 30 to 1,000 mg/m 2 , and the surface treating agent is free from chromium, has a mixing ratio of 20 to 90 wt. % of a fluorine-free titanium compound and 10 to 80 wt. % of alumina, and the surface treating agent has a metal titanium content of 1 to 20 wt. %, wherein the fluorine-free titanium compound is at least one of titanium lactate, ammonium titanium lactate, titanium sulfate, titanium oxysulfate, ammonium titanium sulfate, titanium nitrate, titanium oxynitrate, and ammonium titanium nitrate. 2. The rubber-metal laminated gasket material according to claim 1 , wherein the alumina is alumina sol. 3. The rubber-metal laminated gasket material according to claim 1 , wherein the rubber is fluororubber or nitrile rubber. 4. The rubber-metal laminated gasket material according to claim 1 , which is used as an engine cylinder head gasket. 5. An engine cylinder head gasket using the rubber-metal laminated gasket material according to claim 4 .
Non-permeable · CPC title
Seals; Sealing equipment; Gaskets · CPC title
of {natural rubber or synthetic} rubber · CPC title
on metal layer · CPC title
Polymeric coating · CPC title