Use of quartz plates during growth of single crystal silicon ingots
US-12146236-B2 · Nov 19, 2024 · US
US10266964B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10266964-B2 |
| Application number | US-201515534102-A |
| Country | US |
| Kind code | B2 |
| Filing date | Dec 4, 2015 |
| Priority date | Dec 17, 2014 |
| Publication date | Apr 23, 2019 |
| Grant date | Apr 23, 2019 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
In the present invention, as a bag to store polycrystalline silicon ingots, there is used a bag in which the concentration of paraffinic hydrocarbons in a concentrate of solvent-soluble components obtained by Soxhlet extraction using acetone as a solvent is lower than 300 ppmw as a value measured by GC-MS method; the concentration of antioxidants, lower than 10 ppmw; the concentration of ultraviolet absorbents, lower than 5 ppmw; and the concentration of antistatic agents and surfactants, lower than 50 ppmw. Then, when the polycrystalline silicon ingots are packed, preferably, the polycrystalline silicon ingots are put in the storage bag; thereafter, the storage bag is sealed; further, the storage bag is put and sealed in a linear low-density polyethylene bag containing an antistatic agent or a surfactant added in the bag material.
Opening claim text (preview).
The invention claimed is: 1. A method for packing a polycrystalline silicon ingot, comprising: putting the polycrystalline silicon ingot in a first storage bag; thereafter sealing the first storage bag; further putting the first storage bag in a second storage bag; and sealing the second storage bag, wherein the first storage bag is composed of a first bag material comprising a linear low-density polyethylene, wherein the second storage bag is composed of a second bag material comprising a linear low-density polyethylene and at least one of an antistatic agent and a surfactant, and wherein a concentration of paraffinic hydrocarbons eluted from the first storage bag is lower than 300 ppmw, as measured by subjecting a sheet of 1 g cut-out as a specimen of the first storage bag to the Soxhlet extraction using acetone as the solvent for 8 hours. 2. A method for producing Czochralski (CZ) silicon single crystal, comprising: performing a Czochralski (CZ) single crystal growth process using a polycrystalline silicon ingot put and stored in a first storage bag as a raw material, wherein the first storage bag is composed of a first bag material comprising a linear low-density polyethylene, wherein a concentration of paraffinic hydrocarbons eluted from the first storage bag is lower than 300 ppmw, as determined by obtaining a concentrate by Soxhlet extraction using acetone as a solvent and then measuring the concentration by a gas chromatography-mass spectrometry (GC-MS) method, and wherein a total concentration of organic substances eluted from the first storage bag onto a surface of the polycrystalline silicon ingot is lower than 4 ppbw, as measured by a gas chromatograph-mass spectrometry (GC-MS) method. 3. A method for producing (CZ) silicon single crystal, comprising: performing a Czochralski (CZ) single crystal growth process using a polycrystalline silicon ingot packed by a method according to claim 1 as a raw material. 4. The method according to claim 1 , wherein the first bag material further comprises at least one additive selected from the group consisting of an antioxidant, an ultraviolet absorbent, an antistatic agent, and a surfactant, and wherein when the first bag material contains the antioxidant, a concentration of the antioxidant eluted from the first storage bag is lower than 10 ppmw, as determined by obtaining a concentrate by Soxhlet extraction using acetone as a solvent and then measuring the concentration by the gas chromatography-mass spectrometry (GC-MS) method.
Single-crystal growth by pulling from a melt, e.g. Czochralski method (under a protective fluid C30B27/00) · CPC title
Silicon (forming single crystals or homogeneous polycrystalline material with defined structure C30B) · CPC title
Silicon · CPC title