Reduced point of sale bases for multi-finish paint line and methods for same

US9994722B2 · US · B2

Patent metadata
FieldValue
Publication numberUS-9994722-B2
Application numberUS-201514865704-A
CountryUS
Kind codeB2
Filing dateSep 25, 2015
Priority dateSep 25, 2015
Publication dateJun 12, 2018
Grant dateJun 12, 2018

How to read this patent

A practical reading order for non-experts. Skip the full description unless you need deep technical detail.

  1. Title

    What the patent document calls the invention.

  2. Abstract

    A short plain-language summary of the technical disclosure.

  3. Assignees and inventors

    Who owns or filed the patent and who is credited as inventor.

  4. Key dates

    Filing, priority, publication, and grant dates set the timeline.

  5. First independent claim

    The legal scope of protection — read this for what is actually claimed.

  6. CPC / IPC classifications

    Technology tags used to group this patent with similar filings.

  7. Citations and related patents

    Prior art links and similar publications in this corpus.

Abstract

Official abstract text for this publication.

Disclosed herein is a method for adjusting factory-made tintable paints at the point of sale by adding at least one gloss modifier to the factory-made tintable paints without substantially changing the amount of opacifying pigments in the tintable paints, so that a single color prescription can be used to tint the paints to a single color for any gloss or sheen. Such same color paints should have a color difference of less than 2.0 CIEDE2000 units. Also disclosed is an aqueous gloss reducer that contains mostly a matting agent with substantially no latex resin and substantially no opacifying pigments.

First claim

Opening claim text (preview).

We claim: 1. A method for adjusting a factory-made tintable paint at a point of sale comprising the steps of receiving the factory-made tintable paint in a plurality of containers, wherein each container comprises a first amount of opacifying pigment, adjusting a finish of the factory-made tintable paint by adding at least one of a gloss reducer or a gloss enhancer into at least one container, wherein the gloss reducer comprises a matting agent and wherein the gloss enhancer comprises a latex resin to produce a second tintable paint, wherein a second amount of opacifying pigment in the second tintable paint is substantially the same as the first amount, wherein the gloss reducer comprises from about 25% to about 40% matting agent. 2. The method of claim 1 , wherein the first and second amounts of opacifying pigments are the same. 3. The method of claim 1 , wherein the gloss reducer comprises from about 25% to about 35% matting agent. 4. The method of claim 3 , wherein the gloss reducer comprises from about 30% to about 35% matting agent. 5. The method of claim 1 , wherein the gloss reducer comprises from about 8% to about 14% of rheological modifier. 6. The method of claim 5 , wherein the gloss reducer comprises from about 9% to about 13% of rheological modifier. 7. The method of claim 6 , wherein the gloss reducer comprises from about 10% to about 12% of rheological modifier. 8. The method of claim 1 , wherein the gloss reducer comprises from about 3% to about 7% of surfactants and dispersants. 9. The method of claim 1 , wherein the matting agent comprises a plurality of average sized silica particles. 10. The method of claim 1 , further comprises the step of adding at least one colorant into said at least one container to form a tinted paint. 11. The method of claim 1 , wherein the finish is selected from a group consisting of a high gloss, a semi-gloss, a satin, an eggshell and a flat/matte, wherein the high gloss has a gloss value at 60° between 70 and 85 or higher, wherein the semi-gloss has a gloss value at 60° between 35 and 70, wherein the satin has a gloss value at 60° between 20 and 35, wherein the eggshell has a gloss value at 60° between 10 and 25, and wherein the flat/matte has a gloss value at 60° between 0 and 10. 12. A method for adjusting tintable paint comprising the steps of receiving or preparing the tintable paint, adding at least one of a gloss reducer or a gloss enhancer to the tintable paint to produce a plurality of second tintable paints having different glosses, tinting the plurality of second tintable paints with a single color prescription to produce a plurality of tinted paints, wherein the color difference between any two tinted paints with different glosses is less than about 2.0 CIEDE2000 units. 13. The method of claim 12 , wherein the glosses are selected from a group consisting of a high gloss, a semi-gloss, a satin, an eggshell and a flat/matte, wherein the high gloss has a gloss value at 60° between 70 and 85 or higher, wherein the semi-gloss has a gloss value at 60° between 35 and 70, wherein the satin has a gloss value at 60° between 20 and 35, wherein the eggshell has a gloss value at 60° between 10 and 25, and wherein the flat/matte has a gloss value at 60° between 0 and 10. 14. The method of claim 13 , wherein the color difference between any two tinted paints with different glosses is less than about 1.0 CIEDE2000 unit. 15. The method of claim 14 , wherein the color difference between any two tinted paints with different glosses is less than about 0.67 CIEDE2000 unit. 16. The method of claim 13 , wherein the gloss reducer comprises about 25% to about 40% matting agent. 17. The method of claim 16 , wherein the matting agent comprises a plurality of average sized silica particles.

Assignees

Inventors

Classifications

  • Gloss-reducing agents · CPC title

  • in aqueous medium (C09D17/003, C09D17/004 take precedence) · CPC title

  • Silica · CPC title

  • C09D7/80Primary

    Processes for incorporating ingredients · CPC title

  • C09D5/024Primary

    characterised by the additives · CPC title

Patent family

Related publications grouped by family.

External sources

Frequently asked questions

Answers are generated from the same data shown on this page.

What does patent US9994722B2 cover?
Disclosed herein is a method for adjusting factory-made tintable paints at the point of sale by adding at least one gloss modifier to the factory-made tintable paints without substantially changing the amount of opacifying pigments in the tintable paints, so that a single color prescription can be used to tint the paints to a single color for any gloss or sheen. Such same color paints should ha…
Who is the assignee on this patent?
Columbia Insurance Co
What technology area does this patent fall under?
Primary CPC classification C09D7/80. Mapped technology areas include Chemistry & Metallurgy.
When was this patent published?
Publication date Tue Jun 12 2018 00:00:00 GMT+0000 (Coordinated Universal Time) (B2). Legal status and post-grant events are not shown on this page.
What related patents are in patentsdb?
We list 1 related publication on this page (citations in our corpus or others sharing the same primary CPC).