Porous carbon interlayer for lithium-sulfur battery
US-9246149-B2 · Jan 26, 2016 · US
US9991539B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9991539-B2 |
| Application number | US-201414782184-A |
| Country | US |
| Kind code | B2 |
| Filing date | Apr 29, 2014 |
| Priority date | Apr 29, 2013 |
| Publication date | Jun 5, 2018 |
| Grant date | Jun 5, 2018 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
The present specification provides a polymer electrolyte membrane, a membrane electrode assembly including the polymer electrolyte membrane, and a fuel cell including the membrane electrode assembly.
Opening claim text (preview).
The invention claimed is: 1. A polymer electrolyte membrane comprising a mixed layer that includes an ion migration region and a support having a 3-dimensional network structure, wherein the ion migration region has a structure in which two or more cells including an ion-conducting material border 3 dimensionally, wherein sections of two or more of the cells are present in both a vertical section and a horizontal section of the polymer electrolyte membrane, and the ion migration region includes the ion-conducting material in greater than or equal to 60% by volume and less than or equal to 100% by volume. 2. A polymer electrolyte membrane comprising a mixed layer that includes an ion migration region and a support having a 3-dimensional network structure, wherein the ion migration region has a structure in which two or more cells including an ion-conducting material border 3 dimensionally, wherein sections of two or more of the cells are present in both a vertical section and a horizontal section of the polymer electrolyte membrane, and a volume ratio of the ion-conducting material with respect to a volume of space in the support is greater than or equal to 0.6 and less than or equal to 1 when 1) separating the ion-conducting material from the support by stirring the polymer electrolyte membrane 3 times for 3 hours each at 80° C. in a solvent capable of dissolving the ion-conducting material, 2) casting the solution including the ion-conducting material separated from the support on a substrate, removing the solvent by drying the result for 24 hours at 100° C., and then measuring the volume of the ion-conducting material, and 3) washing the support with methanol, drying the result for 24 hours at 100° C., and then measuring the volume of space in the support. 3. A polymer electrolyte membrane comprising a mixed layer that includes an ion migration region and a support having a 3-dimensional network structure, wherein the ion migration region has a structure in which two or more cells including an ion-conducting material border 3 dimensionally, wherein sections of two or more of the cells are present in both a vertical section and a horizontal section of the polymer electrolyte membrane, and the polymer electrolyte membrane further comprising a pure layer including only the ion-conducting material on an upper surface, a lower surface, or an upper surface and a lower surface of the mixed layer, wherein a volume ratio of the ion-conducting material included in the mixed layer with respect to a volume of space in the support is greater than or equal to 0.6 and less than or equal to 1 when 1) measuring a mass of the polymer electrolyte membrane and measuring a volume of the pure layer, 2) separating the ion-conducting material from the support by stirring the polymer electrolyte membrane 3 times for 3 hours each at 80° C. in a solvent capable of dissolving the ion-conducting material, 3) casting the solution including the ion-conducting material separated from the support on a substrate, removing the solvent by drying the result for 24 hours at 100° C., and then measuring a mass and density of the ion-conducting material, 4) washing the support with methanol, drying the result for 24 hours at 100° C., and then measuring the volume of space in the support, 5) measuring a mass of the pure layer from the density of the ion-conducting material and the volume of the pure layer, and 6) measuring a mass of the ion-conducting material included in the mixed layer through subtracting the mass of the pure layer from the mass of the ion-conducting material, and calculating a volume of the ion-conducting material included in the mixed layer through the mass of the ion-conducting material included in the mixed layer and the density of the ion-conducting material. 4. The polymer electrolyte membrane of claim 1 , wherein the ion migration region is greater than or equal to 40% by volume and less than or equal to 85% by volume with respect to a total volume of the mixed layer. 5. The polymer electrolyte membrane of claim 1 , wherein a thickness of the mixed layer is greater than or equal to 1 μm and less than or equal to 30 μm. 6. The polymer electrolyte membrane of claim 1 further comprising a pure layer including only the ion-conducting material provided on an upper surface, a lower surface, or an upper surface and a lower surface of the mixed layer. 7. The polymer electrolyte membrane of claim 6 , wherein thicknesses of the pure layers provided on any one surface of the mixed layer are each independently greater than 0 μm and less than or equal to 6 μm. 8. The polymer electrolyte membrane of claim 6 , wherein a thickness difference between the pure layers each provided on the upper surface and the lower surface of the mixed layer is 50% or less of a thickness of the mixed layer. 9. The polymer electrolyte membrane of claim 6 , wherein a thickness ratio of the mixed layer and the whole pure layer is from 1:0 to 1:4. 10. The polymer electrolyte membrane of claim 6 , wherein the pure layers provided on any one surface of the mixed layer are each independently laminated in two or more layers, and each layer includes a different ion-conducting material. 11. The polymer electrolyte membrane of claim 1 , which has a total thickness of greater than or equal to 3 μm and less than or equal to 36 μm. 12. The polymer electrolyte membrane of claim 1 , wherein the ion-conducting material includes a hydrocarbon-based material. 13. The polymer electrolyte membrane of claim 12 , wherein the hydrocarbon-based material is a polymer having one or more cation exchangers on a side chain, a ratio of the number of carbon atoms and the number of fluorine atoms included in the polymer is greater than or equal to 1:0 and less than 1:1, and the cation exchanger includes one or more types selected from the group consisting of a sulfonic acid group, a carboxylic acid group, a phosphoric acid group, a phosphonic acid group and derivatives thereof. 14. The polymer electrolyte membrane of claim 1 , which has an RH cycle limit of at least 20,000 cycles. 15. The polymer electrolyte membrane of claim 1 , wherein the ion-conducting material includes one, two or more types selected from the group consisting of a sulfonated benzimidazole polymer, a sulfonated polyimide-based polymer, a sulfonated polyetherimide-based polymer, a sulfonated polyphenylenesulfide-based polymer, a sulfonated polysulfone-based polymer, a sulfonated polyethersulfone-based polymer, a sulfonated polyetherketone-based polymer, a sulfonated polyether-etherketone-based polymer, a sulfonated polyphenylquinoxaline-based polymer, and a polymer in which a sulfonated partial fluorine-based is introduced. 16. The polymer electrolyte membrane of claim 1 , wherein the support includes a hydrocarbon-based material. 17. The polymer electrolyte membrane of claim 1 , wherein the support includes a semi-crystalline polymer. 18. The polymer electrolyte membrane of claim 1 , wherein the support includes polyolefin, polyamide, polyester, polyacetal (or polyoxymethylene), polysulfide, polyvinyl alcohol, copolymers thereof and combinations thereof. 19. The polymer electrolyte membrane of claim 1 , wherein an average of maximum diameters of the cells is greater than or equal to 0.25 μm and less than or equal to 0.4 μm, and a standard deviation of maximum diameters of the cells is greater than or equal to 0.05 μm and less than or equal to 0.2 μm. 20. The polymer electrolyte membrane of claim 1 , wherein the cells are laminated
Fuel cells · CPC title
characterised by the chemical composition of the porous support · CPC title
Cross-Sectional Technologies · mapped topic
halogenated, e.g. sulfonated polyvinylidene fluorides · CPC title
in the form of layered products, e.g. coatings · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.