Method for making electrode foils having reduced particle detachment and reduced leakage current
US-2015211145-A1 · Jul 30, 2015 · US
US9991056B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9991056-B2 |
| Application number | US-201514849064-A |
| Country | US |
| Kind code | B2 |
| Filing date | Sep 9, 2015 |
| Priority date | Sep 9, 2015 |
| Publication date | Jun 5, 2018 |
| Grant date | Jun 5, 2018 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A process and apparatus are presented for cleaning the tunnels of an electrochemically etched anode foil. The apparatus includes a tank, a fluid inlet and a fluid outlet, and one or more tranducers. The tank is designed to receive a plurality of cartridges, each of the plurality of cartridges having a reservoir and being designed to hold a metal foil. The fluid inlet and fluid outlet are coupled with at least one of the plurality of cartridges, and are designed to introduce and expel, respectively, a liquid from the reservoir within at least one of the plurality of cartridges. The one or more transducers are coupled to at least one wall of each reservoir, the one or more transducers being designed to sonicate the liquid within each reservoir at a frequency less than 300 Hz.
Opening claim text (preview).
What is claimed is: 1. A method of processing a metal foil, comprising: electrochemically etching the metal foil to form a plurality of tunnels in the metal foil; disposing the etched metal foil in a widening solution comprising PSSA, wherein the widening solution is configured to widen the plurality of tunnels in the metal foil; removing the etched metal foil from the widening solution; and sonicating the metal foil in a liquid at a frequency less than 300 Hz, wherein the sonicating removes excess PSSA from the plurality of tunnels. 2. The method of claim 1 , wherein the metal foil is an aluminum foil. 3. The method of claim 1 , wherein the widening solution further comprises 10% by weight aluminum nitrate and 0.5% by weight nitric acid. 4. The method of claim 1 , wherein a pH of the widening solution is maintained below three. 5. The method of claim 1 , wherein the liquid is de-ionized water. 6. The method of claim 5 , wherein the de-ionized water is recirculated during the sonicating. 7. The method of claim 1 , wherein the sonicating comprises vibrating a first wall on one side of a reservoir, and vibrating a second wall on an opposite side of the reservoir. 8. The method of claim 7 , wherein the first wall and the second wall are vibrated out-of-phase with each other. 9. The method of claim 7 , wherein the first wall and the second wall have a thickness between 1 and 5 micrometers. 10. The method of claim 1 , wherein the widening solution comprises between 250 and 350 ppm of PSSA.
Etching · CPC title
Etched foil electrodes · CPC title
based on aluminium · CPC title
Processes of manufacture · CPC title
by sonic or ultrasonic vibrations · CPC title