Method and apparatus for making a gypsum board
US-2024033972-A1 · Feb 1, 2024 · US
US9975808B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9975808-B2 |
| Application number | US-201414268557-A |
| Country | US |
| Kind code | B2 |
| Filing date | May 2, 2014 |
| Priority date | May 2, 2014 |
| Publication date | May 22, 2018 |
| Grant date | May 22, 2018 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
An ultra-light, pourable, self-drying cementitious product with improved density control and ultra-low water demand is provided. Compositions and methods for making the products are provided as well, including compositions and methods with ultra-low water demand.
Opening claim text (preview).
What is claimed is: 1. An ultra-light pourable, self-leveling cementitious composition comprising: 60% to 80% of a 50:50 combination of cement and gypsum component; 0.1% to 10% of a surfactant selected from the group consisting of an anionic surfactant, non-ionic surfactant, cationic surfactant, amphoteric surfactant and any mixture thereof; 1% to 30% of a filler selected from the group consisting of coated perlite, uncoated perlite, shale, glass spheres, expanded polystyrene balls (EPS) and any combination thereof; and water; wherein the ratio of water to dry components is in the range from 0.17 to 0.30; and wherein the wet density of the composition is in the range from 20 to 40 lbs/ft 3 . 2. The ultra-light cementitious composition of claim 1 further comprising at least one of the following: a superplasticizer, hydration reaction accelerator, hydration reaction retarder and polypropylene fibers. 3. The ultra-light cementitious composition of claim 1 , wherein the surfactant comprises a mixture of sodium laureth sulfate, sodium lauryl sulfate and alkyl dimethyl amine oxide. 4. The ultra-light cementitious composition of claim 1 , wherein the surfactant is a stock solution comprising 1-5% ethyl alcohol, 10-30% sodium laureth sulfate and sodium lauryl sulfate and 3-7% alkyl dimethyl amine oxide. 5. A method of making an ultra-light cementitious product, the method comprising: preparing the composition of claim 1 , wherein the density of the composition is adjusted by controlling the amount of foam added; pouring the composition into a cast or on to a surface; allowing the poured composition to self-level; and servicing the poured product. 6. The method of claim 5 , wherein the product is selected from the group consisting of doors, wall panels, garage door panels, wall partition systems, ceiling panels, gun safes and file cabinets. 7. The method of claim 5 , wherein the wet density is adjusted in the range 20-40 lbs/ft 3 . 8. The method of claim 5 , wherein all dry components except for the filler are mixed together first and added to liquid components and the filler is then added in portions to achieve a wet density in the range 20-40 lbs/ft 3 . 9. A method of making a flooring, the method comprising: preparing a first ultra-light cementitious composition according to claim 1 with the first compressive strength and pouring the composition over a substrate; preparing a second cementitious composition with the second compressive strength, wherein the second compressive strength is higher than the first strength; pouring the second cementitious composition over the first composition. 10. The method of claim 9 , wherein the second cementitious composition is an ultra-light cementitious composition according to claim 1 . 11. The ultra-light cementitious composition of claim 1 , wherein the surfactant is a mixture of at least one anionic surfactant and at least one nonionic surfactant. 12. The ultra-light cementitious composition of claim 1 , wherein the composition further comprises fibers selected from the group consisting of organic fibers, inorganic fibers and any combination thereof. 13. The ultra-light cementitious composition of claim 12 , wherein the fibers are selected from the group consisting of fiberglass fibers, acrylic fibers, cellulose fibers, polypropylene fibers and any combination thereof.
containing calcium sulfate cements {(gypsum-paper plates E04C)} · CPC title
Mortar or concrete mixtures with an unusual water/cement ratio · CPC title
Gypsum-paper board like materials · CPC title
White cement · CPC title
Flooring materials · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.