A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
The invention provides a composition for the production of a fiber having organic solvent resistance, a fiber obtained by spinning the composition, and a biocompatible material containing the fiber. The composition contains (A) a polymer compound containing a unit structure represented by the formula (1) wherein each symbol is as described herein, (B) a crosslinking agent, (C) an acid compound, and (D) a solvent.
Opening claim text (preview).
The invention claimed is: 1. A method of producing a fiber, comprising spinning a composition comprising (A) a polymer compound consisting of monomer units represented by formula (1) that are the same or different wherein R 1 is a hydrogen atom or a methyl group, Q 1 is an ester bond or an amide bond, R 2 is an alkyl group having 1-10 carbon atoms or an aromatic hydrocarbon group having 6-10 carbon atoms, wherein at least one hydrogen atom is substituted by a hydroxy group, (B) a crosslinking agent, (C) an acid compound, and (D) a solvent to form a fiber. 2. The method according to claim 1 , wherein the spinning is electrospinning. 3. The method according to claim 1 , further comprising heating the fiber at 70-300° C. 4. A fiber produced by the method according to claim 1 . 5. A biocompatible material comprising the fiber according to claim 4 .
of esters containing halogen, nitrogen, sulfur, or oxygen atoms in addition to the carboxy oxygen · CPC title
the material being a polymer solution or dispersion (D01D5/0053 takes precedence) · CPC title
Electro-spinning (non-woven fabrics produced by electro-spinning D04H1/728) · CPC title
used for fibers · CPC title
by electro-spinning {(electro-spinning methods and apparatus D01D5/0007)} · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.