Process for making crosslinked cable insulation using high melt strength ethylene-based polymer made in a tubular reactor and optionally modified with a branching agent
US-11912852-B2 · Feb 27, 2024 · US
US9938395B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9938395-B2 |
| Application number | US-201615208853-A |
| Country | US |
| Kind code | B2 |
| Filing date | Jul 13, 2016 |
| Priority date | Dec 11, 2015 |
| Publication date | Apr 10, 2018 |
| Grant date | Apr 10, 2018 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A transparent composite material composition, comprises, based on a total amount of the transparent composite material: 90 to 99% by weight of a thermosetting urethane acrylate resin; and 1 to 10% by weight of an organic hydroperoxide initiator. Such a transparent composite material composition exhibits superior properties such as superior transparency, impact resistance, scratch resistance, and weather resistance while realizing weight reduction.
Opening claim text (preview).
What is claimed is: 1. A method of preparing a transparent composite material, the method comprising: preparing a thermosetting urethane acrylate resin; preparing a transparent composite material composition, based on a total amount of the transparent composite material composition, by adding 1% to 10% by weight of an organic hydroperoxide initiator to 90% to 99% by weight of the thermosetting urethane acrylate resin; and hardening and molding the transparent composite material composition, wherein the thermosetting urethane acrylate resin is a halogen-substituted urethane acrylate resin. 2. The method according to claim 1 , wherein the organic hydroperoxide initiator is at least one selected from the group consisting of perbutyl peroxide, di-t-butyl peroxide, t-butylcumyl peroxide, dicumyl peroxide, di-(2,4-dichlorobenzoyl)-peroxide, dibenzoyl peroxide, di(2-tert-butylperoxyisopropyl)benzene, t-butyl peroxybenzoate, 1,1-di-(t-butylperoxy)-3,3,5-trimethylcyclohexane, and 2,5-dimethyl-2,5di(t-butylperoxy)-hexane. 3. The method according to claim 1 , wherein the hardening is carried out by heating to 45 to 95° C. 4. The method according to claim 1 , wherein the hardening is carried out through UV irradiation.
containing condensed aromatic rings · CPC title
having fluorine atoms · CPC title
Protective means for window, e.g. additional panel or foil, against vandalism, dirt, wear, shattered glass, etc. · CPC title
having heteroatoms other than oxygen · CPC title
being toluene diisocyanate including isomer mixtures · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.