Method of producing a printed image on a pre-treated, low-porous or non-porous medium
US-9505024-B2 · Nov 29, 2016 · US
US9937524B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9937524-B2 |
| Application number | US-201013516838-A |
| Country | US |
| Kind code | B2 |
| Filing date | Dec 24, 2010 |
| Priority date | Dec 29, 2009 |
| Publication date | Apr 10, 2018 |
| Grant date | Apr 10, 2018 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Provided is a method of manufacturing a flexographic printing plate with which it is possible to prevent plate surface contamination even in the printing for long time. A method for manufacturing a flexographic printing plate, characterized in that, a liquid containing an amino-modified silicone compound is made to contact with a flexographic printing plate containing a latex having gelation degree of not less than 50% by mass. Said latex occupies preferably not less than 30% by mass of the printing resin plate, and amino group equivalent of the amino-modified silicone compound is preferably not less than 500 g/mol.
Opening claim text (preview).
The invention claimed is: 1. A method for manufacturing a flexographic printing plate, characterized in that, a liquid containing an amino-modified silicone compound is made to contact with a flexographic printing plate containing a latex having gelation degree of not less than 50% by mass, wherein the amino-modified silicone compound having amino group equivalent of not less than 1800 g/mol is used, and wherein dot bridging at initial stage of printing and after printing of the flexographic printing plate is not observed. 2. The manufacturing method according to claim 1 , wherein content of the latex having gelation degree of not less than 50% by mass is not less than 30% by mass in a printing plate resin composition. 3. The manufacturing method according to claim 1 , wherein the flexographic printing plate further contains an emulsifier. 4. The manufacturing method according to claim 3 , wherein the emulsifier is an anionic surfactant. 5. The manufacturing method according to claim 1 , wherein the latex has the gelation degree of not less than 70% by mass. 6. The manufacturing method according to claim 1 , wherein the amino-modified silicone compound having amino group equivalent of 1800 g/mol to 20,000 g/mol. 7. The manufacturing method according to claim 1 , wherein the amino-modified silicone compound having amino group equivalent of 1800 g/mol to 10,000 g/mol.
to obtain a surface receptive to ink or other liquid (B05D5/02, {B41M5/52} take precedence) · CPC title
Preparing for use and conserving printing surfaces · CPC title
the binders being polymers obtained by reactions only involving carbon-to-carbon unsaturated bonds, e.g. vinyl polymers · CPC title
Silicon-containing polymers · CPC title
Treatment with inorganic or organometallic reagents after imagewise removal · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.