Composite active material, solid state battery and method for producing composite active material
US-2015311507-A1 · Oct 29, 2015 · US
US9929403B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9929403-B2 |
| Application number | US-201514640772-A |
| Country | US |
| Kind code | B2 |
| Filing date | Mar 6, 2015 |
| Priority date | Mar 19, 2014 |
| Publication date | Mar 27, 2018 |
| Grant date | Mar 27, 2018 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A method of producing an active material powder includes (i) an attachment step of obtaining a powder including an active material particle, which stores and releases lithium ions at a potential of 4.5 V or higher based on Li, and a coating layer precursor, which is attached to a surface of the active material particle, by attaching an alkoxide solution containing lithium ions and niobium ions to the surface of the active material particle and drying the attached alkoxide solution; and (ii) a heating step of forming a coating layer on the surface of the active material particle by heating the powder obtained in the attachment step to be within a temperature range of 120° C. to 200° C.
Opening claim text (preview).
What is claimed is: 1. A method of producing an active material powder, the method comprising: attaching an alkoxide solution containing lithium ions and niobium ions to a surface of an active material particle and drying the attached alkoxide solution to obtain a powder; and heating the powder within a temperature range of 120° C. to 200° C. to form a coating layer on the surface of the active material particle, wherein the active material particle contains Mn and stores and releases lithium ions at a potential of 4.5 V or higher based on Li. 2. The method according to claim 1 , wherein the alkoxide solution attached to the surface of the active material particle is dried while the alkoxide solution is attached to the surface of the active material particle. 3. The method according to claim 1 , wherein the active material particle contains LiNi 0.5 Mn 1.5 O 4 or LiNi 1/3 Co 1/3 Mn 1/3 O 2 . 4. The method according to claim 1 , wherein the active material particle contains LiNi 0.5 Mn 1.5 O 4 .
Selection of inactive substances as ingredients for active masses, e.g. binders, fillers · CPC title
one phase coated with the other · CPC title
Surface area · CPC title
of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy · CPC title
as layered products · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.