Duplex ferritic austenitic stainless steel
US-2016115574-A1 · Apr 28, 2016 · US
US9869002B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9869002-B2 |
| Application number | US-201514962424-A |
| Country | US |
| Kind code | B2 |
| Filing date | Dec 8, 2015 |
| Priority date | Dec 11, 2014 |
| Publication date | Jan 16, 2018 |
| Grant date | Jan 16, 2018 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
There is provided a method for manufacturing a duplex stainless steel sheet having reduced inclusions through argon oxygen decarburization (AOD), ladle treatment (LT), and twin roll strip casting. The method includes deoxidizing molten steel using silicon (Si) during the AOD, wherein the molten steel has a silicon (Si) content of 0.55 wt % to 0.75 wt % at the end of the AOD.
Opening claim text (preview).
What is claimed is: 1. A method for manufacturing a duplex stainless steel sheet, the method comprising: argon oxygen decarburization (AOD), ladle treatment (LT), and twin roll strip casting, wherein the AOD comprises: deoxidizing molten steel with silicon (Si), wherein the molten steel has a silicon (Si) content of 0.55 wt % to 0.75 wt % at an end of the AOD, and wherein the duplex stainless steel sheet comprises, by wt %, carbon (C): 0.02% to 0.06%, silicon (Si): 0.55% to 0.75%, manganese (Mn): 2.8% to 3.2%, phosphorus (P): 0.035% or less, sulfur (S): 0.003% or less, chromium (Cr): 19.0% to 21.0%, nickel (Ni): 0.5% to 1.5%, copper (Cu): 0.3% to 1.2%, nitrogen (N): 0.2% to 0.28%, and a balance of iron (Fe) and inevitable impurities. 2. The method of claim 1 , wherein in the AOD, slag has a basicity of 2.2 to 2.5. 3. The method of claim 1 , wherein the molten steel has a tapping temperature of 1680° C. to 1710° C. in the AOD.
Deoxidising, e.g. killing · CPC title
of stainless steel · CPC title
with more than 1.5% by weight of manganese · CPC title
Treatment of slags covering the steel bath, e.g. for separating slag from the molten metal · CPC title