Component repair using brazed surface textured superalloy foil
US-2015375346-A1 · Dec 31, 2015 · US
US9863019B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9863019-B2 |
| Application number | US-201514789442-A |
| Country | US |
| Kind code | B2 |
| Filing date | Jul 1, 2015 |
| Priority date | Sep 4, 2014 |
| Publication date | Jan 9, 2018 |
| Grant date | Jan 9, 2018 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A high-strength Ni-base alloy having favorable corrosion resistance, high strength, and high ductility, around room temperature is provided. A high-strength Ni-base alloy includes: in % by mass, less than 0.01% of C, not more than 0.5% of Si, not more than 0.5% of Mn, 15 to 25% of Cr. 1.0 to 5.0% of Mo or Mo+0.5W, 0.2 to 0.8% of Al, 1.0 to 2.0% of Ti, 3.00 to 3.80% of Nb, not more than 30% of Fe, and 0.0007 to 0.010% of Mg; Ni; and impurities. A value represented by Mg/S is not less than 0.7, and an A value is not less than 0.015 and less than 0.027, the A value being represented by A value=Al/(Al+1.77(Ti−1.36C)+3.44(Nb−5.1C)).
Opening claim text (preview).
What is claimed is: 1. A Ni-base alloy consisting of: in % by mass, less than 0.01% of C, not more than 0.5% of Si, not more than 0.5% of Mn, 15 to 25% of Cr, 1.0 to 5.0% of Mo or Mo+0.5W, 0.2 to 0.8% of Al, 1.0 to 2.0% of Ti, 3.00 to 3.80% of Nb, not more than 30% of Fe, and 0.0007 to 0.010% of Mg; Ni; and impurities, wherein a value represented by Mg/S is not less than 0.7, and an A value is not less than 0.015 and less than 0.027, the A value being represented by: A value=Al/(Al+1.77(Ti−1.36C)+3.44(Nb−5.1C)); and a total of an area ratio of a region where a plate-like intermetallic compound exists alone and an area ratio of a region where a plate-like intermetallic compound phase and a γ phase exist in a lamellar manner, in a cross-sectional microstructure after age-hardening treatment, is not more than 12.5%. 2. The Ni-base alloy according to claim 1 , wherein the A value is 0.015 to 0.025. 3. The Ni-base alloy according to claim 1 , wherein the total of the area ratios is not more than 10.0%.
with the maximum Cr content being at least 10% but less than 20% · CPC title
with the maximum Cr content being at least 20% but less than 30% · CPC title
of nickel or cobalt or alloys based thereon · CPC title
with chromium · CPC title