Window member and manufacturing method thereof
US-2024336031-A1 · Oct 10, 2024 · US
US9862864B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9862864-B2 |
| Application number | US-201313949955-A |
| Country | US |
| Kind code | B2 |
| Filing date | Jul 24, 2013 |
| Priority date | Jan 27, 2011 |
| Publication date | Jan 9, 2018 |
| Grant date | Jan 9, 2018 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A swelling tape for filling a gap and a method of filling a gap are provided. The swelling tape can be applied within the gap having a fluid to realize a 3D shape thereby filling the gap, and be used to fix a subject forming the gap as necessary.
Opening claim text (preview).
What is claimed is: 1. A swelling tape for filling a gap, comprising: a substrate layer that deforms along a longitudinal direction when coming in contact with a fluid; and a pressure-sensitive adhesive layer formed on one surface of the substrate layer in a direction parallel to a longitudinal direction of the substrate layer, wherein the substrate layer is a layer selected from the group consisting of: a cast layer of a composition consisting essentially of 30 parts by weight to 99 parts by weight of an energy ray-polymerizable acrylate compound and 1 part by weight to 70 parts by weight of a radical-polymerizable diluents; a cast layer of a composition comprising a polyol and an isocyanate compound; a layer comprising thermoplastic polyurethane; and a layer comprising a cellulose acetate resin or a cellulose alkylate resin, wherein the substrate layer forms a three-dimensional structure when coming in contact with a fluid, wherein the three-dimensional structure includes a shape protruding along the vertical direction and wherein a plurality of the shapes are included in the three-dimensional structure, and wherein the substrate layer has a strain of at least 10% in a longitudinal direction according to Equation 1: Strain in Longitudinal direction=( L 2 −L 1 )/ L 1 ×100, [Equation1] wherein L 1 is an initial length of the substrate layer before the substrate layer comes in contact with the fluid; and L 2 is a length of the substrate layer, which is measured after the substrate layer comes in contact with the fluid at room temperature or 60° C. for 24 hours. 2. The swelling tape of claim 1 , wherein the pressure-sensitive adhesive layer has a peel strength of 100 gf/25 mm or more at room temperature, which is measured at a peel rate of 5 mm/sec and a peel angle of 180° to a glass plate or any one subject that forms a gap. 3. The swelling tape of claim 1 , wherein the pressure-sensitive adhesive layer includes an acrylic pressure-sensitive adhesive, a urethane pressure-sensitive adhesive, an epoxy pressure-sensitive adhesive, a silicon pressure-sensitive adhesive, or a rubber pressure-sensitive adhesive. 4. A method of filling a gap, which is formed by a first substrate and a second substrate spaced apart from the first substrate, comprising: attaching a pressure-sensitive adhesive layer of the swelling tape according to claim 1 to the first substrate or the second substrate; and deforming the substrate layer in a longitudinal direction by bringing the substrate layer of the swelling tape in contact with a fluid. 5. The method of claim 4 , wherein one of the first and second substrates is an electrode assembly and the other is a can receiving the assembly. 6. The swelling tape of claim 1 , wherein the substrate layer is the cast layer of the composition comprising the polyol and the isocyanate compound, and wherein the polyol includes an alkylene glycol, a dialkylene glycol, a benzenediol, a benzenetriol, a dialcohol amine, a trialcohol amine, arabitol, mannitol, isomalt, glycerol, xylitol, sorbitol, maltitol, erythritol, ribitol, dulcitol, lactitol, threitol, iditol or polyglycitol.
Devices for making primary cells · CPC title
Processes of manufacture in general · CPC title
Vinyl resins, e.g. polyvinyl chloride [PVC] · CPC title
Laminated material (metallised plastics C09J7/22) · CPC title
in the substrate · CPC title
Related publications grouped by family.