System and method for forming a metal beverage container using blow molding
US-9321093-B2 · Apr 26, 2016 · US
US9849501B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9849501-B2 |
| Application number | US-201415026049-A |
| Country | US |
| Kind code | B2 |
| Filing date | Sep 30, 2014 |
| Priority date | Sep 30, 2013 |
| Publication date | Dec 26, 2017 |
| Grant date | Dec 26, 2017 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A system and method of forming a metal container with a featured sidewall may include providing a blow molded metal container. The metal container may be positioned into a mold inclusive of at least one sidewall feature. The metal container may be blow molded again to cause the at least one sidewall feature to be created in the sidewall of the container as defined by the mold. In one embodiment, a sidewall of the metal container may be at least partially annealed. The sidewall feature may include a portion of a profile of a sporting good, such as a baseball, embossed feature (e.g., word), logo, or otherwise. The metal container may be a shaped metal container.
Opening claim text (preview).
What is claimed: 1. A method of forming at least one molded feature in a container, said method comprising: accessing a metal container with a sidewall; at least partially annealing the sidewall of the metal container; positioning the metal container into a mold inclusive of at least one mold feature; and blow molding the metal container to cause the at least one molded feature to be created in the sidewall of the metal container as defined by the at least one mold feature in the mold. 2. The method according to claim 1 , wherein accessing the metal container includes providing a partially formed metal container. 3. The method according to claim 1 , wherein accessing the metal container includes providing a fully formed metal container. 4. The method according to claim 1 , wherein at least partially annealing the sidewall includes heating the sidewall to a temperature that causes metal grains of the sidewall to transition to a reduced stress state from an existing stress state. 5. The method according to claim 1 , wherein at least partially annealing the sidewall includes at least partially annealing a localized portion of the sidewall. 6. The method according to claim 1 , wherein positioning the metal container in the mold includes moving a plurality of mold pieces about the metal container, the mold pieces, when integrated or in contact with one another, having a profile that substantially matches a profile of the metal container with the exception of the at least one mold feature of the mold. 7. The method according to claim 1 , wherein the at least one mold feature includes a portion of a profile of a sporting good. 8. The method according to claim 1 , wherein the at least one mold feature includes an embossed feature. 9. The method according to claim 8 , wherein accessing the metal container with the sidewall comprises accessing a metal container formed by blow molding. 10. The method according to claim 1 , wherein the metal in the molded feature in the sidewall has a different hardness than metal in the sidewall surrounding the molded feature. 11. The method according to claim 1 , wherein accessing the metal container includes providing a shaped metal container in a shape of a bottle. 12. A system for forming a metal container with a featured sidewall, said system comprising: a heater configured to at least partially anneal the featured sidewall of the metal container; a mold inclusive of at least one mold feature, and adapted to receive a blow molded metal container with a sidewall; and a blowing mechanism configured to blow mold the metal container again to cause the at least one mold feature to create at least one molded feature in the sidewall of the metal container. 13. The system according to claim 12 , wherein the mold is configured to accept a partially formed metal container. 14. The system according to claim 12 , wherein the mold is configured to accept a fully formed metal container. 15. The system according to claim 12 , wherein the heater is configured to at least partially anneal the sidewall to a temperature that causes metal grains of the sidewall to transition to a reduced stress state from an existing stress state. 16. The system according to claim 12 , wherein the heater is configured to heat the at least partially annealed sidewall in a localized portion of the sidewall. 17. The system according to claim 12 , wherein the mold includes a plurality of mold pieces configured to be formed about the metal container, the mold pieces, when integrated or in contact with one another, having a profile that substantially matches a profile of the metal container with the exception of the at least one mold feature of the mold. 18. The system according to claim 12 , wherein the at least one mold feature includes a portion of a profile of a sporting good.
Deforming bodies having a closed end · CPC title
Locally embossing the walls of formed can bodies (B44B5/00, B44C1/24, B44C3/085 take precedence; bulging B21D51/2646) · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.