Manufacturing method of aluminum-based article with multi-angle visual color change characteristics
US-2024344229-A1 · Oct 17, 2024 · US
US9845547B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9845547-B2 |
| Application number | US-201514621008-A |
| Country | US |
| Kind code | B2 |
| Filing date | Feb 12, 2015 |
| Priority date | Oct 24, 2014 |
| Publication date | Dec 19, 2017 |
| Grant date | Dec 19, 2017 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A method for surface treatment of aluminum alloys for forms an oxidation film in the aluminum alloys for casting by adding a metallic anion compound to an electrolytic solution. The method can prevent cracks from occurring on a surface of the aluminum alloys for casting at the time of applying an anodizing method.
Opening claim text (preview).
What is claimed is: 1. A method for surface treatment of aluminum alloys for casting, comprising: forming an oxidation film in the aluminum alloys for casting by adding a metallic anion compound to an electrolytic solution, wherein the electrolytic solution is prepared using any one material selected from sulfuric acid and oxalic acid as a base, and wherein the metallic anion compound is NaAlO 2 . 2. The method of claim 1 , wherein the aluminum alloys for casting includes Si ranging from 4.0 to 24.0 wt %, and the oxidation film has a thickness which is set to be equal to or more than 5 μm. 3. The method of claim 2 , comprising steps of: coupling anions of the metallic anion compound included in the electrolytic solution with cracks formed on a surface of the aluminum alloys for casting by controlling a range of voltage, current, time, and temperature. 4. The method of claim 3 , wherein the voltage is controlled to be within a range of 10 to 200 V, the current is controlled to be within a range of 0.2 to 10 A/cm 2 , and the time is controlled to be within a range of 1 to 24 h, and the metallic anion compound is added within a range of 0.02 to 0.4 M.