Optical film with pressure sensitive adhesive on both sides and method for producing image display device using thereof, and method for suppressing curl of optical film with pressure sensitive adhesive on both sides

US9841545B2 · US · B2

Patent metadata
FieldValue
Publication numberUS-9841545-B2
Application numberUS-201514876946-A
CountryUS
Kind codeB2
Filing dateOct 7, 2015
Priority dateOct 15, 2014
Publication dateDec 12, 2017
Grant dateDec 12, 2017

How to read this patent

A practical reading order for non-experts. Skip the full description unless you need deep technical detail.

  1. Title

    What the patent document calls the invention.

  2. Abstract

    A short plain-language summary of the technical disclosure.

  3. Assignees and inventors

    Who owns or filed the patent and who is credited as inventor.

  4. Key dates

    Filing, priority, publication, and grant dates set the timeline.

  5. First independent claim

    The legal scope of protection — read this for what is actually claimed.

  6. CPC / IPC classifications

    Technology tags used to group this patent with similar filings.

  7. Citations and related patents

    Prior art links and similar publications in this corpus.

Abstract

Official abstract text for this publication.

The optical film with a pressure sensitive adhesive on both sides includes a first pressure sensitive adhesive layer having a thickness of 3 μm to 30 μm on first main surface of an optical film, and a second pressure sensitive adhesive layer having a thickness of 50 μm or more on second main surface of the optical film. A first protective sheet and a second protective sheet are releasably attached on the first pressure sensitive adhesive layer and the second pressure sensitive adhesive layer, respectively. The residual stress of the second pressure sensitive adhesive layer S 2 (N/cm 2 ), the thickness of the first protective sheet Y (μm); and the thickness of the second protective sheet Z (μm) satisfy the following relationship: 20≦Y≦80; 45≦Z; and Y+0.17 Z+10.6 S 2 ≧63.

First claim

Opening claim text (preview).

What is claimed is: 1. An optical film with a pressure sensitive adhesive on both sides, which is to be disposed between a front transparent plate or a touch panel and an image display cell, wherein the optical film with a pressure sensitive adhesive on both sides comprises: an optical film including a polarizing plate; a first pressure sensitive adhesive layer provided on first main surface of the optical film, which is to be bonded to an image display cell; and a second pressure sensitive adhesive layer provided on second main surface of the optical film, which is to be bonded to a transparent plate or a touch panel, a first protective sheet is releasably attached on the first pressure sensitive adhesive layer, and a second protective sheet is releasably attached on the second pressure sensitive adhesive layer, the first pressure sensitive adhesive layer has a thickness of 3 μm to 30 μm, and a storage elastic modulus of 0.02 MPa to 2 MPa at a temperature of 23° C., and the second pressure sensitive adhesive layer has a thickness of 50 μm or more, and where a residual stress of the second pressure sensitive adhesive layer is S 2 (N/cm 2 ); the thickness of the first protective sheet is Y (μm); and the thickness of the second protective sheet is Z (μm), the absolute values of S 2 , Y and Z satisfy the following relationship: 20≦ Y≦ 80; 45≦ Z ; and Y+ 0.17 Z+ 10.6 S 2 ≧63, wherein the residual stress is a tensile stress as measured by a tensile stress relaxation test under conditions of a temperature of 23° C., a strain of 300%, and a relaxation time of 180 seconds. 2. The optical film with a pressure sensitive adhesive on both sides according to claim 1 , wherein each of a tensile elastic modulus of the first protective sheet and a tensile elastic modulus of the second protective sheet is 1 GPa to 6 GPa. 3. The optical film with a pressure sensitive adhesive on both sides according to claim 1 , wherein each of the first protective sheet and the second protective sheet is a biaxially stretched polyester film. 4. The optical film with a pressure sensitive adhesive on both sides according to claim 1 , wherein the thickness Z of the second protective sheet is larger than the thickness Y of the first protective sheet. 5. The optical film with a pressure sensitive adhesive on both sides according to claim 1 , wherein the second pressure sensitive adhesive layer contains a photocurable component. 6. A method for producing an image display device, comprising: providing an optical film with a pressure sensitive adhesive on both sides which comprises an optical film, a first pressure sensitive adhesive layer on first main surface of the optical film, a second pressure sensitive adhesive layer on second surface of the optical film, a first protective sheet releasably attached on the first pressure sensitive adhesive layer, and a second protective sheet releasably attached on the second pressure sensitive adhesive layer; a first bonding step of peeling off the first protective sheet attached on the first pressure sensitive adhesive layer, and then bonding a first main surface of the optical film and an image display cell to each other with the first pressure sensitive adhesive layer interposed therebetween; and a second bonding step of peeling off the second protective sheet attached on the second pressure sensitive adhesive layer, and then bonding a second surface side of the optical film and a front transparent plate or a touch panel to each other with the second pressure sensitive adhesive layer interposed therebetween, wherein the optical film includes a polarizing plate, the first pressure sensitive adhesive layer has a thickness of 3 μm to 30 μm, and a storage elastic modulus of 0.02 MPa to 2 MPa at a temperature of 23° C., the second pressure sensitive adhesive layer has a thickness of 50 μm or more, and where a residual stress of the second pressure sensitive adhesive layer is S 2 (N/cm 2 ); the thickness of the first protective sheet is Y (μm); and the thickness of the second protective sheet is Z (μm), the absolute values of S 2 , Y and Z satisfy the following relationship: 20≦ Y≦ 80; 45≦ Z ; and Y+ 0.17 Z+ 10.6 S 2 ≧63, wherein the residual stress is a tensile stress as measured by a tensile stress relaxation test under conditions of a temperature of 23° C., a strain of 300%, and a relaxation time of 180 seconds. 7. The method for producing an image display device according to claim 6 , wherein the second pressure sensitive adhesive layer contains a photocurable component, and after the second bonding step, an active ray is applied from the front transparent plate or touch panel side to cure the second pressure sensitive adhesive layer. 8. A method for suppressing curl of an optical film with a pressure sensitive adhesive on both sides, wherein the optical film with a pressure sensitive adhesive on both sides is to be disposed between a front transparent plate or a touch panel and an image display cell, and comprises: an optical film including a polarizing plate; a first pressure sensitive adhesive layer provided on a surface of the optical film, which is to be bonded to an image display cell; and a second pressure sensitive adhesive layer provided on second surface of the optical film, which is to be bonded to a transparent plate or a touch panel, a first protective sheet is releasably attached on the first pressure sensitive adhesive layer, and a second protective sheet is releasably attached on the second pressure sensitive adhesive layer, the first pressure sensitive adhesive layer has a thickness of 3 μm to 30 μm, and a storage elastic modulus of 0.02 MPa to 2 MPa at a temperature of 23° C., the second pressure sensitive adhesive layer has a thickness of 50 μm or more, and where a residual stress of the second pressure sensitive adhesive layer is S 2 (N/cm 2 ); the thickness of the first protective sheet is Y (μm); and the thickness of the second protective sheet is Z (μm), S 2 , Y and Z are set to satisfy the following relationship: 20≦ Y≦ 80; 45≦ Z ; and Y+ 0.17 Z+ 10.6 S 2 ≧63, wherein the residual stress is a tensile stress as measured by a tensile stress relaxation test under conditions of a temperature of 23° C., a strain of 300%, and a relaxation time of 180 seconds.

Assignees

Inventors

Classifications

  • G02B5/3033Primary

    in the form of a thin sheet or foil, e.g. Polaroid · CPC title

  • in the substrate · CPC title

  • characterised by the substrate of the release liner · CPC title

  • for the production of liquid crystal displays · CPC title

  • Pressure-sensitive adhesives [PSA] · CPC title

Patent family

Related publications grouped by family.

External sources

Frequently asked questions

Answers are generated from the same data shown on this page.

What does patent US9841545B2 cover?
The optical film with a pressure sensitive adhesive on both sides includes a first pressure sensitive adhesive layer having a thickness of 3 μm to 30 μm on first main surface of an optical film, and a second pressure sensitive adhesive layer having a thickness of 50 μm or more on second main surface of the optical film. A first protective sheet and a second protective sheet are releasably attac…
Who is the assignee on this patent?
Nitto Denko Corp
What technology area does this patent fall under?
Primary CPC classification G02B5/3033. Mapped technology areas include Physics.
When was this patent published?
Publication date Tue Dec 12 2017 00:00:00 GMT+0000 (Coordinated Universal Time) (B2). Legal status and post-grant events are not shown on this page.
What related patents are in patentsdb?
We list 8 related publications on this page (citations in our corpus or others sharing the same primary CPC).