Integrated circuit arrangement, device and gas detection method
US-9140678-B2 · Sep 22, 2015 · US
US9834637B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9834637-B2 |
| Application number | US-201615095842-A |
| Country | US |
| Kind code | B2 |
| Filing date | Apr 11, 2016 |
| Priority date | Apr 11, 2016 |
| Publication date | Dec 5, 2017 |
| Grant date | Dec 5, 2017 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A process of forming a macromolecular block copolymer includes forming a first high molecular weight polymer using a first extruder of an extruder system that includes multiple extruders. The first extruded high molecular weight polymer has a first length terminating at a joiner of the extruder system and has a first set of material properties along the first length. The process also includes forming a second high molecular weight polymer using a second extruder of the extruder system. The second extruded high molecular weight polymer has a second length terminating at the joiner of the extruder system and has a second set of material properties along the second length. The process further includes bonding the first extruded high molecular weight polymer to the second extruded high molecular weight polymer to form a macromolecular block copolymer having a first segment of the first length and a second segment of the second length.
Opening claim text (preview).
The invention claimed is: 1. A process of forming a block copolymer, the process comprising: forming, by polymerization, a first extruded polymer using a first extruder of an extruder system that includes multiple extruders, the first extruded polymer having a first length terminating at a joiner of the extruder system, wherein the first extruded polymer has a first set of rigidity, flexibility, and chemical properties along the first length; forming, by polymerization, a second extruded polymer using a second extruder of the extruder system, the second extruded polymer having a second length terminating at the joiner of the extruder system, wherein the second extruded polymer has a second set of rigidity, flexibility, and chemical properties along the second length; and bonding covalently at least a portion of the first extruded polymer to the second extruded polymer to form a block copolymer having a first segment of the first length and a second segment of the second length, wherein at least one of the first extruded polymer and the second extruded polymer includes side-chain functional groups for chemically bonding the block copolymer to a polymeric matrix material. 2. The process of claim 1 , wherein the side-chain functional groups include amine groups, norbornene groups, hydroxyl groups, or a combination thereof. 3. The process of claim 1 , wherein the polymeric matrix material includes ethylene propylene diene monomer (EPDM) rubber, and wherein the side-chain functional groups include norbornene groups. 4. A process of forming a block copolymer, the process comprising: forming, by polymerization, an extruded polystyrene (PS) polymer using a first extruder of an extruder system that includes multiple extruders, the extruded PS polymer having a first length terminating at a joiner of the extruder system; forming, by polymerization, an extruded linear low density polyethylene (LLDPE) polymer using a second extruder of the extruder system, the extruded LLDPE polymer having a second length terminating at the joiner; and bonding covalently at least a portion of the extruded PS polymer to the extruded LLDPE polymer to form a PS-LLDPE block copolymer having a first segment of the first length and a second segment of the second length, the first segment having a first rigidity along the first length and a second rigidity of the second segment along the second length, wherein the extruded PS polymer and the extruded LLDPE polymer include side-chain functional groups for chemically bonding the PS-LLDPE block copolymer to a polymeric matrix material. 5. The process of claim 4 , further comprising: forming, by polymerization, a second extruded PS polymer using the first extruder, the second extruded PS polymer having a third length terminating at the joiner; and bonding covalently at least a portion of the second extruded PS polymer to the extruded LLDPE polymer to form a third segment of the PS-LLDPE block copolymer, the third segment having the first rigidity along the third length. 6. The process of claim 4 , wherein the polymeric matrix material includes ethylene propylene diene monomer (EPDM) rubber, and wherein the side-chain functional groups include norbornene groups.
Joining {or sealing} of preformed parts {, e.g. welding of plastics materials}; Apparatus therefor {(general aspects of processes or apparatus for joining preformed parts B29C66/00; using porous material formed by internal pressure generated therein for joining preformed parts B29C44/1228, B29C44/326)} · CPC title
Feeding {of the material to be moulded}, e.g. into a mould cavity {(B29C39/08 takes precedence; using a material distribution system to two or more fixed injection moulds B29C45/125)} · CPC title
Operations & Transport · mapped topic
from unsaturated polycondensates · CPC title
Polymers of compounds having carbon-to-carbon double bonds · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.