Welded joint and automobile member
US-2024093708-A1 · Mar 21, 2024 · US
US9822432B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9822432-B2 |
| Application number | US-201113511015-A |
| Country | US |
| Kind code | B2 |
| Filing date | Oct 4, 2011 |
| Priority date | Jan 11, 2011 |
| Publication date | Nov 21, 2017 |
| Grant date | Nov 21, 2017 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A magnesium alloy that forms a stable protective film on the surface of molten metal, having excellent ignition resistance restricting natural ignition of a chip thereof as well as having excellent strength and ductility, so that the Mg alloy can be melted and cast in the air or a common inert atmosphere. The magnesium alloy includes, by weight, 7.0% or greater but less than 11% of Al, 0.05% to 2.0% of Ca, 0.05% to 2.0% of Y, greater than 0% but not greater than 6.0% of Zn, and the balance of Mg, and the other unavoidable impurities. The total content of the Ca and the Y is equal to or greater than 0.1% but less than 2.5% of the total weight of the magnesium alloy.
Opening claim text (preview).
The invention claimed is: 1. A magnesium alloy manufactured by melt casting, the magnesium alloy consisting of, by weight, 7.0% or greater but less than 9.5% of Al, 0.05% to 0.58% of Ca, 0.05% to 0.4% of Y, greater than 0% but less than 1.2% of Zn, greater than 0% but not greater than 1.0% of Mn, a balance of Mg, and other unavoidable impurities, and an oxide layer including a CaO and Y 2 O 3 layer disposed on the magnesium alloy, and a MgO and CaO layer disposed on the CaO and Y 2 O 3 layer, wherein a total content of the Ca and the Y is equal to or greater than 0.1% but less than 0.98% of a total weight of the magnesium alloy. 2. The magnesium alloy of claim 1 , wherein the total content of the Ca and the Y is equal to or greater than 0.1% but less than 0.7% of the total weight of the magnesium alloy.
Casting aluminium or magnesium {(no material; see B22D21/007)} · CPC title
with aluminium as the next major constituent · CPC title
Special casting characterised by the nature of the product (B22D15/02, B22D17/16, B22D19/00 take precedence; casting stereotype plates B41D3/00) · CPC title
by melting {(C22C1/1036 takes precedence)} · CPC title
with zinc or cadmium as the next major constituent · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.