Process to prepare lower olefins
US-2024182385-A1 · Jun 6, 2024 · US
US9822313B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9822313-B2 |
| Application number | US-201515511047-A |
| Country | US |
| Kind code | B2 |
| Filing date | Sep 21, 2015 |
| Priority date | Sep 23, 2014 |
| Publication date | Nov 21, 2017 |
| Grant date | Nov 21, 2017 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
Form liquid product stream that has a C 13 to C 20 hydrocarbon content of less than 5.0 wt % based upon a total weight of the liquid product stream via a process that includes contacting synthesis gas with a sulfurized Zeolite Socony Mobil-5 catalyst. The sulfurized Zeolite Socony Mobil-5 catalyst can include ZSM-5, cobalt, an alkali metal, sulfur, and a reduction promoter.
Opening claim text (preview).
What is claimed: 1. A process for producing a liquid product stream that has a C 13 to C 20 hydrocarbon content of less than 5.0 wt % based upon a total weight of the liquid product stream, the process comprising: contacting synthesis gas with a sulfurized Zeolite Socony Mobil-5 catalyst, wherein the sulfurized Zeolite Socony Mobil-5 catalyst includes cobalt and a sulfur doped Zeolite Socony Mobil-5 support, with the sulfur being incorporated via sulfate ions, the cobalt being present in an amount within a range of from 1 to 25 wt % based upon a dry weight of the sulfurized Zeolite Socony Mobil-5 catalyst, the sulfur being present in an amount within a range of from 0.01 to 1.00 wt %, based upon a dry weight of the sulfurized Zeolite Socony Mobil-5 catalyst, the conditions consisting essentially of a temperature within a range of from 150 to 300° C., a pressure within a range of from 5 to 40 bar, and a gas hourly space velocity within a range of from 100 to 10000 h −1 . 2. The process of claim 1 , wherein the sulfurized Zeolite Socony Mobil-5 catalyst includes an alkali metal. 3. The process of claim 2 , wherein the alkali metal is within a range of from 0.01 to 4.50 wt % based upon a dry weight of the sulfurized ZSM-5 catalyst. 4. The process of claim 2 , wherein the alkali metal is sodium. 5. The process of claim 1 , wherein the sulfurized Zeolite Socony Mobil-5 catalyst includes a reduction promoter. 6. The process of claim 5 , wherein the reduction promoter is within a range of from 0.01 to 5.00% based upon a dry weight of the sulfurized ZSM-5 catalyst. 7. The process of claim 6 , wherein the reduction promoter is ruthenium. 8. The process of claim 1 , wherein the liquid product stream has a C 5 -C 12 hydrocarbon content of at least 25 wt % based upon a total weight of the liquid product stream.