Nickel-free green pigment
US-2015353706-A1 · Dec 10, 2015 · US
US9822015B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-9822015-B2 |
| Application number | US-201013513885-A |
| Country | US |
| Kind code | B2 |
| Filing date | Dec 2, 2010 |
| Priority date | Dec 7, 2009 |
| Publication date | Nov 21, 2017 |
| Grant date | Nov 21, 2017 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
The present invention provides a method of producing a lithium mixed metal oxide, a lithium mixed metal oxide and a nonaqueous electrolyte secondary battery. The method includes a step of calcining a mixture of one or more compounds of M wherein M is one or more elements selected from the group consisting of nickel, cobalt and manganese, and a lithium compound, in the presence of one or more inactive fluxes selected from the group consisting of a fluoride of A, a chloride of A, a carbonate of A, a sulfate of A, a nitrate of A, a phosphate of A, a hydroxide of A, a molybdate of A and a tungstate of A, wherein A is one or more elements selected from the group consisting of Na, K, Rb, Cs, Ca, Mg, Sr and Ba. The lithium mixed metal oxide contains nickel, cobalt and manganese, has a BET specific surface area of from 3 m 2 /g to 15 m 2 /g, and has an average particle diameter within a range of 0.1 μm or more to less than 1 μm, the diameter determined by a laser diffraction scattering method.
Opening claim text (preview).
The invention claimed is: 1. A lithium mixed metal oxide comprising nickel, cobalt, and manganese, having a BET specific surface area of from 5.1 m 2 /g to 15 m 2 /g, and having an average particle diameter within a range of 0.1 μm or more and 0.8 μm or less, the diameter determined by a laser diffraction scattering method, wherein the average particle diameter is the average diameter of primary particles and secondary particles in the lithium mixed metal oxide; wherein the lith…
Chemistry & Metallurgy · mapped topic
Chemistry & Metallurgy · mapped topic
Electricity · mapped topic
Chemistry & Metallurgy · mapped topic
Electricity · mapped topic
Related publications grouped by family.
Free tools are coming soon. Tell us what you want to track and we'll notify you.
Answers are generated from the same data shown on this page.